Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.00600 - 0.0160 cm/cm | 0.00600 - 0.0160 in/in | Average value: 0.00843 cm/cm Grade Count:14 |
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are.. |
|||
Linear Mold Shrinkage, Transverse | 0.00600 - 0.0190 cm/cm | 0.00600 - 0.0190 in/in | Average value: 0.0130 cm/cm Grade Count:5 |
Overview of materials for Polyetheretherketone, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Linear Mold Shrinkage, Transverse | 0.00600 - 0.0300 cm/cm | 0.00600 - 0.0300 in/in | Average value: 0.0143 cm/cm Grade Count:12 |
Overview of materials for Acetal Copolymer, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Linear Mold Shrinkage, Transverse | 0.00600 - 0.0140 cm/cm | 0.00600 - 0.0140 in/in | Average value: 0.00811 cm/cm Grade Count:18 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an.. |
|||
Linear Mold Shrinkage, Transverse | 0.00600 - 0.00700 cm/cm @Temperature 80.0 - 80.0 °C |
0.00600 - 0.00700 in/in @Temperature 176 - 176 °F |
Average value: 0.00650 cm/cm Grade Count:2 |
Overview of materials for Nylon 6, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Linear Mold Shrinkage, Transverse | 0.00600 - 0.00600 cm/cm @Temperature 80.0 - 80.0 °C |
0.00600 - 0.00600 in/in @Temperature 176 - 176 °F |
Average value: 0.00600 cm/cm Grade Count:6 |
Overview of materials for Nylon 6, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E.. |
|||
Linear Mold Shrinkage, Transverse | 0.00600 - 0.0200 cm/cm | 0.00600 - 0.0200 in/in | Average value: 0.0125 cm/cm Grade Count:10 |
Overview of materials for Nylon 66, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu.. |
|||
Linear Mold Shrinkage, Transverse | 0.00600 - 0.0200 cm/cm | 0.00600 - 0.0200 in/in | Average value: 0.0109 cm/cm Grade Count:33 |
Overview of materials for Nylon 66, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu.. |
|||
Linear Mold Shrinkage, Transverse | 0.00600 - 0.00900 cm/cm | 0.00600 - 0.00900 in/in | Average value: 0.00817 cm/cm Grade Count:6 |
Overview of materials for Nylon 6-3 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Linear Mold Shrinkage, Transverse | 0.00600 - 0.00800 cm/cm @Temperature 80.0 - 80.0 °C |
0.00600 - 0.00800 in/in @Temperature 176 - 176 °F |
Average value: 0.00695 cm/cm Grade Count:20 |
Overview of materials for Nylon 6, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Linear Mold Shrinkage, Transverse | 0.00600 - 0.0140 cm/cm | 0.00600 - 0.0140 in/in | Average value: 0.00970 cm/cm Grade Count:6 |
Overview of materials for Nylon 66/6, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, Mineral Reinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Linear Mold Shrinkage, Transverse | 0.00600 - 0.0150 cm/cm | 0.00600 - 0.0150 in/in | Average value: 0.0115 cm/cm Grade Count:33 |
Overview of materials for Polyether Block Amide (PEBA) This property data is a summary of similar materials in the MatWeb database for the category "Polyether Block Amide (PEBA)". Each property range of values reported is minimum and maximum values of a.. |