Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0010 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0030 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® HFD4413 PC (Asia Pacific) Lexan* HFD4413 is a 30% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
Linear Mold Shrinkage, Transverse | 0.00090 - 0.0030 cm/cm | 0.00090 - 0.0030 in/in | ASTM D955 |
PolyOne Edgetek® UR2-40CF/000 BLACK Polyurethane, Unspecified (PUR, Unspecified) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Linear Mold Shrinkage, Transverse | 0.0010 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0030 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LGK5030 PC (Asia Pacific) Glass reinforced. Flame retardant. |
|||
Linear Mold Shrinkage, Transverse | 0.0015 - 0.0030 cm/cm | 0.0015 - 0.0030 in/in | |
LATI Larton GCE/600 PPS, Glass/Mineral Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa .. |
|||
Linear Mold Shrinkage, Transverse | 0.0015 - 0.0030 cm/cm | 0.0015 - 0.0030 in/in | |
LATI Larton GCE/650 PPS, Glass/Mineral Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa .. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0030 cm/cm | 0.0020 - 0.0030 in/in | |
LATI Larton K/20 PPS, 20% Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Linear Mold Shrinkage, Transverse | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4 |
Lanxess Durethan® ECO BV 30 H2 900500 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, injection molding, heat-ageing stabilized, contains 30% pre-consumer recycled materialInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Transverse | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4 |
Lanxess Durethan® ECO BV 35 H2 900500 Nylon 6, 35% Glass Fiber PA 6, 35% glass fibers, injection molding, heat-ageing stabilized, contains 30% pre-consumer recycled materialInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0030 cm/cm | 0.0020 - 0.0030 in/in | |
LATI Larton L K/20 L-PPS, 20% Carbon Fiber Reinforced Linear Polyphenylene Sulfide (L-PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle.. |
|||
Linear Mold Shrinkage, Transverse | 0.0015 - 0.0030 cm/cm | 0.0015 - 0.0030 in/in | |
LATI Laticonther 80 GCE/650 PPS, Glass/Mineral Reinforced High thermal conductivity product based on Polyphenylene Sulfide (PPS). Glass fibers / Mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformatio.. |
|||
Linear Mold Shrinkage, Transverse | 0.0015 - 0.0030 cm/cm | 0.0015 - 0.0030 in/in | |
LATI Latilon 28D K/40 PC, 40% Carbon Fiber Reinforced Polycarbonate (PC) based compound. Carbon fiber. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided b.. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0030 cm/cm @Time 86400 sec |
0.0020 - 0.0030 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRILOY DF204 PC LNP* LUBRILOY* DF204 is a compound based on Polycarbonate resin containing 20% Glass Fiber, Proprietary Lubricant. Added feature of th is grade is: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.0010 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0030 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP STAT-KON DX10315C PC (Asia Pacific) LNP* Stat-Kon* DX10315C is carbon fiber filled polycarbonate composite with good stiffness, good flow ability, ESD safety, and high level of cleanliness for the most demanding application. This comp.. |
|||
Linear Mold Shrinkage, Transverse | 0.0010 - 0.0030 cm/cm @Time 86400 sec |
0.0010 - 0.0030 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON DX13320C PC COPOLYMER (Asia Pacific) LNP* Statkon DX13320C is ultra clean polycarbonate/carbon fiber compound with high modulus, good flow ability, easy mold release, and high level of cleanliness for the most demanding application. A .. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0030 cm/cm @Time 86400 sec |
0.0020 - 0.0030 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Stat-kon EE008E PEI (Asia Pacific) LNP STAT-KON* EE008E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Asia Pacif.. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0030 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP STAT-KON Lexan_LCF1506 PC (Europe-Africa-Middle East) LNP* Stat-kon* Lexan_LCF1506 is a 15% carbon fiber, 6% PTFE reinforced polycarbonate. |
|||
Linear Mold Shrinkage, Transverse | 0.0015 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0015 - 0.0030 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC1010 PPE+HIPS (Europe-Africa-Middle East) LNP* Stat-kon* HMC1010 compound is a 10% Carbon fiber reinforced. Static dissipative. Nonbrominated, nonchlornated flame retardant system. UL94 V-1 rated. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0030 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC1508 PPE+HIPS (Europe-Africa-Middle East) LNP* Stat-kon* Noryl_HMC1508 compound is a static dissipative NORYL resin. |
|||
Linear Mold Shrinkage, Transverse | 0.0015 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0015 - 0.0030 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC3008A PPE+HIPS (Europe-Africa-Middle East) LNP* Stat-kon* Noryl_HMC3008A compound is a 30% glass/mineral/carbon fiber reinforced resin; static dissipative; 250F (120C) HDT. Tight tolerance molding. |
|||
Linear Mold Shrinkage, Transverse | 0.0015 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0015 - 0.0030 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC3008A PPE+PS LNP* Stat-kon* Noryl_HMC3008A compound is a 30% glass/mineral/carbon fiber reinforced resin; static dissipative; 250F (120C) HDT. Tight tolerance molding. |
|||
Linear Mold Shrinkage, Transverse | 0.0010 - 0.0030 cm/cm @Time 86400 sec |
0.0010 - 0.0030 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP D351 PC (Asia Pacific) LNP* Thermocomp* D351 (experimental grade name as EXTC8143) is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus,.. |
|||
Linear Mold Shrinkage, Transverse | 0.0010 - 0.0030 cm/cm @Time 86400 sec |
0.0010 - 0.0030 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP EXTC8143 PC (Asia Pacific) LNP* Thermocomp* EXTC8143 is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good ductility, No.. |
|||
Linear Mold Shrinkage, Transverse | 0.0010 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0030 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK5030 PC LNP* Thermocomp* Lexan_LGN5030 compound is a glass reinforced. Flame retardant. |
|||
Linear Mold Shrinkage, Transverse | 0.0010 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0030 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK5030 PC (Asia Pacific) Glass reinforced. Flame retardant. |
|||
Linear Mold Shrinkage, Transverse | 0.0010 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0030 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® HFD4412 PC Lexan* HFD4412 is a 20% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
Linear Mold Shrinkage, Transverse | 0.0010 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0030 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® HFD4412 PC (Europe-Africa-Middle East) Lexan* HFD4412 is a 20% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
Linear Mold Shrinkage, Transverse | 0.0010 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0030 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® HFD4413 PC (Europe-Africa-Middle East) Lexan* HFD4413 is a 30% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
Linear Mold Shrinkage, Transverse | 0.0010 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0030 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® HFD4412 PC (Asia Pacific) Lexan* HFD4412 is a 20% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0030 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP STAT-KON Lexan_LCF1506 PC (Asia Pacific) 15% carbon fiber, 6% PTFE reinforced polycarbonate. |