Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0018 cm/cm
0.0018 in/in
ISO 294-4, 2577
Lanxess Pocan® B 4225 000000 PBT, 20% Glass Fiber
PBT, 20% glass fibers, injection molding, flame retardant
Linear Mold Shrinkage, Transverse 0.0018 cm/cm
0.0018 in/in
ISO 294-4
Solvay Specialty Polymers Kalix® 5950 HFFR Polyamide, High Performance (HPPA), 50% Glass Fiber
Kalix® 5950 HFFR is a halogen-free, flame retardant (UL-94 V0 at 0.4 mm), highly reinforced polyamide material specifically formulated for high strength and stiffness applications where good impa..