Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0018 cm/cm | 0.0018 in/in | ISO 294-4, 2577 |
Lanxess Pocan® B 4225 000000 PBT, 20% Glass Fiber PBT, 20% glass fibers, injection molding, flame retardant |
|||
Linear Mold Shrinkage, Transverse | 0.0018 cm/cm | 0.0018 in/in | ISO 294-4 |
Solvay Specialty Polymers Kalix® 5950 HFFR Polyamide, High Performance (HPPA), 50% Glass Fiber Kalix® 5950 HFFR is a halogen-free, flame retardant (UL-94 V0 at 0.4 mm), highly reinforced polyamide material specifically formulated for high strength and stiffness applications where good impa.. |