Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 95000 cP @Shear Rate 300 1/s, Temperature 190 °C |
95000 cP @Shear Rate 300 1/s, Temperature 374 °F |
Apparent Dynamic Viscosity |
Dow DOWLEX™ IP-50 High Density Polyethylene DOWLEX® IP-50 resin is an improved processing high density polyethylene resin with controlled molecular weight distribution designed for thin wall food containers. This resin is recommended for flo.. |