Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Viscosity = 83186 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 83186 cP

@Shear Rate 500 1/s,
Temperature 290 °C
83186 cP

@Shear Rate 500 1/s,
Temperature 554 °F
ISO 11403-1 -2
DuPont Performance Polymers Zytel® FE5382 BK276 Nylon 612  (Unverified Data**)
33% Glass Reinforced Polyamide 612 Developed for Electrical and Electronics Applications Zytel FE5382 BK276 is a 33% glass fiber reinforced heat stabilized black polyamide 612 resin developed for el..
Copyright © lookpolymers.com All Rights Reserved