Polymer Property : Viscosity = 64000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 64000 cP

@Shear Rate 1000 1/s,
Temperature 190 °C
64000 cP

@Shear Rate 1000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
Dow DOWLEX™ 2553 Linear Low Density Polyethylene, Narrow MW Distribution
DOWLEX® 2553 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer good environmental stress crack resistance and impact strength with excellent stiffness for hou..
Viscosity 64000 cP

@Shear Rate 5000 1/s,
Temperature 315 °C
64000 cP

@Shear Rate 5000 1/s,
Temperature 599 °F
ISO 11403-1 -2
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66  (Unverified Data**)
Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe..
Viscosity 64000 cP

@Shear Rate 5000 1/s,
Temperature 260 °C
64000 cP

@Shear Rate 5000 1/s,
Temperature 500 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® LW9020 NC010 PBT+ASA  (Unverified Data**)
20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. ..
Viscosity 64000 cP

@Shear Rate 5000 1/s,
Temperature 295 °C
64000 cP

@Shear Rate 5000 1/s,
Temperature 563 °F
ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G30HSL BK039B Nylon 66  (Unverified Data**)
30% Glass Reinforced Heat Stabilized Polyamide 66 Information provided by DuPont Performance Polymers