Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 40000 - 50000 cP @Temperature 25.0 °C |
40000 - 50000 cP @Temperature 77.0 °F |
TA4202A |
Permabond TA4202 Toughened Acrylic Adhesive PERMABOND® TA4202 is a 2-part, 1:1 toughened acrylic adhesive. It can be used to bond a wide variety of materials including metals, plastics, GRP, ceramics, wood and other substrates. It is conveni.. |
|||
Viscosity | 40000 - 50000 cP @Temperature 25.0 °C |
40000 - 50000 cP @Temperature 77.0 °F |
TA4202B |
Permabond TA4202 Toughened Acrylic Adhesive PERMABOND® TA4202 is a 2-part, 1:1 toughened acrylic adhesive. It can be used to bond a wide variety of materials including metals, plastics, GRP, ceramics, wood and other substrates. It is conveni.. |
|||
Viscosity | 15000 - 50000 cP @Temperature 25.0 °C |
15000 - 50000 cP @Temperature 77.0 °F |
TA4592B, at 2.5 rpm vibration |
Permabond TA4592 Toughened Acrylic Adhesive PERMABOND® TA4592 is a two component structural acrylic adhesive ideal for bonding magnets and ferrites for electric motors on fast-moving production lines. Permabond® TA4592 provides high strengt.. |