Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 230000 - 230000 cP @Temperature 250 - 250 °C |
230000 - 230000 cP @Temperature 482 - 482 °F |
Average value: 230000 cP Grade Count:2 |
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25.. |
|||
Viscosity | 230000 - 230000 cP @Shear Rate 1000 - 1000 1/s |
230000 - 230000 cP @Shear Rate 1000 - 1000 1/s |
Average value: 230000 cP Grade Count:2 |
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25.. |
|||
Viscosity | 230000 cP @Shear Rate 1000 1/s, Temperature 315 °C |
230000 cP @Shear Rate 1000 1/s, Temperature 599 °F |
|
DSM Arnite® AV2 390 XT PET GF50 50% Glass Reinforced, Applications with extremely narrow tolerances |
|||
Viscosity | 230000 cP @Shear Rate 1000 1/s, Temperature 315 °C |
230000 cP @Shear Rate 1000 1/s, Temperature 599 °F |
|
DSM Arnite® AV2 390 XL PET GF50 50% Glass Reinforced, Low outgassing |