Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1000 - 2000 cP @Temperature 40.0 °C |
1000 - 2000 cP @Temperature 104 °F |
|
Abatron AboCast/AboCure 8109-11 All-purpose, structural dielectric resin. Better thermal and chemical properties than 8109-8, but requires heat cure. Melts at 70-80°C and remains liquid (supercooled) for many hours at RT.Process.. |
|||
Viscosity | 1000 - 2000 cP @Temperature 40.0 °C |
1000 - 2000 cP @Temperature 104 °F |
|
Abatron AboCast/AboCure 8109-13 Liquid hardener version of AboCast/AboCure 8109-11.Processing: 100/23 pbw; Potlife: 3-5 h/20°C (68°F), 1-3 h/40°C (105°F), 0.5-1 h/60°C (140°F); mix at RT; cures in: 30 mins/60°C (140°F), 45.. |
|||
Viscosity | 1000 - 2000 cP @Temperature 25.0 °C |
1000 - 2000 cP @Temperature 77.0 °F |
|
Abatron AboCast/AboCure 8109-7 Processing: 100/80 pbw; Potlife: 6-7 days/20°C (68°F), 12-24 h/40°C (105°F), 0.75-7 h /60°C (140°F); mix at 50-80°C (120-175°F); cures in: 1 h/100°C (212°F) + 4 h/150°C (300°F) postcure... |