Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Viscosity = 2.83e+7 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 2.83e+7 cP

@Shear Rate 0.100 1/s,
Temperature 190 °C
2.83e+7 cP

@Shear Rate 0.100 1/s,
Temperature 374 °F
0.1 rad/sec; ARES Rheometer
Dow Engage® ENR 7380.00 Ethylene-Butene Copolymer
Description: ENR 7380.00 is a revolutionary new ethylene-butene copolymer with higher molecular weight, better toughness, and higher melt strength than other commercially available polyolefin elasto..