Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 150 cP @Shear Rate 100 1/s, Temperature 280 °C |
150 cP @Shear Rate 100 1/s, Temperature 536 °F |
|
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p.. |
|||
Viscosity | 150 cP @Shear Rate 100 1/s, Temperature 280 °C |
150 cP @Shear Rate 100 1/s, Temperature 536 °F |
|
Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Viscosity | 150 cP @Shear Rate 100 1/s, Temperature 280 °C |
150 cP @Shear Rate 100 1/s, Temperature 536 °F |
|
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Viscosity | 150 cP @Shear Rate 100 1/s, Temperature 300 °C |
150 cP @Shear Rate 100 1/s, Temperature 572 °F |
|
Solvay TECHNYL® A 221 PA66, DRY Description TECHNYL ® A 221 is an unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. It is available in natural colors. Benef.. |
|||
Viscosity | 150 cP @Shear Rate 1000 1/s, Temperature 260 °C |
150 cP @Shear Rate 1000 1/s, Temperature 500 °F |
|
Solvay TECHNYL® C 218 V 30 PA6, 30% glass fiber, DRY Description: TECHNYL® C 218 V30 is a polyamide 6, heat stabilized, reinforced with 30% of glass fiber, for injection molding. This product is available in black color.Benefits: The product offers.. |
|||
Viscosity | 150 cP @Shear Rate 100 1/s, Temperature 280 °C |
150 cP @Shear Rate 100 1/s, Temperature 536 °F |
|
Solvay TECHNYL® A 218W V30 Natural PA66, 30% glass fiber, DRY Description: TECHNYL® A 218W V30 Nat is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The produc.. |
|||
Viscosity | 150 cP @Temperature 25.0 °C |
150 cP @Temperature 77.0 °F |
|
BASF Pluracol® P1010 Specialty Polyol Description: Pluracol® P polyols are a series of five polypropylene glycols formed by adding propylene oxide to a propylene glycol nucleus. Pluracol P1010, P2010 and 1044 (formerly P4010) are used .. |