Polymer Property : Viscosity = 11000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 11000 cP

@Shear Rate 11200 1/s,
Temperature 200 °C
11000 cP

@Shear Rate 11200 1/s,
Temperature 392 °F
ASTM D3835
PolyOne Dynalloy™ 8900-60 Thermoplastic Elastomer (TPE)
Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen..
Viscosity 11000 cP

@Temperature 25.0 °C
11000 cP

@Temperature 77.0 °F
Resin; STM 1
Lord Adhesives Thermosetâ„¢ UR-329 Two Component Urethane Potting Compound
Lord UR-329 is a flexible, two-component, room temperature curing, urethane, encapsulating compound. UR-329 maintains low hardness and modulus over a wide temperature range, which imparts minimal st..
Viscosity 11000 - 15000 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
11000 - 15000 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Gwent Electronic Materials D2070412D3 Polymer Dielectric
Green colored screen printable polymer dielectric, suitable for defining electrode areas and forms a protective layer over the electrode tracking during immersion of the electrode. The formulation ..
Viscosity 11000 cP

@Temperature 20.0 °C
11000 cP

@Temperature 68.0 °F
BASF Palamoll® 656 Polymeric Plasticizer
Description: Palamoll® 656 is a high viscosity polymeric plasticizer that is compatible with PVC. It is based on adipic acid and polyhydric alcohols. It is resistant to oils, fats, aliphatic hydro..