Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 100000 cP @Temperature 25.0 °C |
100000 cP @Temperature 77.0 °F |
at 20 rpm vibration |
Permabond MH196 Anaerobic Gasketmaker Permabond® MH196 is an anaerobic material designed for making “formed in situ” gaskets between metal surfaces. It is capable of replacing a wide range of conventional gaskets, thereby offering po.. |
|||
Viscosity | 100000 cP @Temperature 25.0 °C |
100000 cP @Temperature 77.0 °F |
ET538B, Polyamine Hardener |
Permabond ET538 Epoxy Resin PERMABOND ET538 is a structural, room temperature curing epoxy adhesive that has excellent adhesion to a wide variety of surfaces such as wood, metal, ceramics and many plastic and composite materia.. |
|||
Viscosity | 100000 cP @Shear Rate 5000 1/s, Temperature 230 °C |
100000 cP @Shear Rate 5000 1/s, Temperature 446 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500AF Acetal (POM)
(Unverified Data**) 20% Teflon® Fiber Filled Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500AF is a medium viscosity acetal homopolymer resin containing 20% Teflon PTFE fibers. It is desi.. |
|||
Viscosity | 100000 cP @Shear Rate 5000 1/s, Temperature 205 °C |
100000 cP @Shear Rate 5000 1/s, Temperature 401 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG400MTD BLA079 Acetal (POM)
(Unverified Data**) Metal Detectable Medium Viscosity Acetal Copolymer Developed for Food Contact Applications Delrin FG400MTD BLA079 is a metal filled medium viscosity acetal copolymer for injection molding. It is det.. |
|||
Viscosity | 100000 cP @Shear Rate 500 1/s, Temperature 300 °C |
100000 cP @Shear Rate 500 1/s, Temperature 572 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 103HSL NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103HSL NC010 is a heat stabilized lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Viscosity | 100000 cP @Frequency 1000 Hz, Temperature 277 °C |
100000 cP @Frequency 1000 Hz, Temperature 531 °F |
|
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Dry, 50% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Viscosity | 100000 cP @Shear Rate 1.00 1/s, Temperature 270 °C |
100000 cP @Shear Rate 1.00 1/s, Temperature 518 °F |
|
DSM Arnite® T06 204 XL PBT Low Viscosity, Injection Molding, Low outgassing |