Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1.10e+6 cP @Shear Rate 67.0 1/s, Temperature 200 °C |
1.10e+6 cP @Shear Rate 67.0 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne OnFlex™ HFFR 310-01 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 310-01 is a non-halogen flame retardant material designed for cable jackets. New Product. Commercial specifications have not been established. - Non-halogen flame retardant - UL62 comp.. |
|||
Viscosity | 1.10e+6 - 1.10e+6 cP @Temperature 190 - 190 °C |
1.10e+6 - 1.10e+6 cP @Temperature 374 - 374 °F |
Average value: 1.10e+6 cP Grade Count:1 |
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Film Grade". Each property range of values reported is minimum and m.. |
|||
Viscosity | 1.10e+6 - 1.10e+6 cP @Shear Rate 50.0 - 50.0 1/s |
1.10e+6 - 1.10e+6 cP @Shear Rate 50.0 - 50.0 1/s |
Average value: 1.10e+6 cP Grade Count:1 |
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Film Grade". Each property range of values reported is minimum and m.. |