Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1.00e+6 - 2.00e+6 cP @Temperature 190 - 190 °C |
1.00e+6 - 2.00e+6 cP @Temperature 374 - 374 °F |
Average value: 1.24e+6 cP Grade Count:5 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade". Each property range of values reported.. |
|||
Viscosity | 1.00e+6 - 2.00e+6 cP @Shear Rate 50.0 - 50.0 1/s |
1.00e+6 - 2.00e+6 cP @Shear Rate 50.0 - 50.0 1/s |
Average value: 1.24e+6 cP Grade Count:5 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade". Each property range of values reported.. |
|||
Viscosity | 1.00e+6 cP @Shear Rate 0.100 1/s, Temperature 260 °C |
1.00e+6 cP @Shear Rate 0.100 1/s, Temperature 500 °F |
|
DSM Akulon® F230-C PA6 Medium Viscosity, Extrusion, Injection Molding |
|||
Viscosity | 1.00e+6 cP @Shear Rate 0.100 1/s, Temperature 280 °C |
1.00e+6 cP @Shear Rate 0.100 1/s, Temperature 536 °F |
|
DSM Akulon® F232 PA6 Medium/High Viscosity, Extrusion Grade |
|||
Viscosity | 1.00e+6 cP @Shear Rate 1.00 1/s, Temperature 270 °C |
1.00e+6 cP @Shear Rate 1.00 1/s, Temperature 518 °F |
|
DSM Arnite® TV4 261 SF PBT-GF30 FR(17) 30% Glass Reinforced, Flame Retardant, High Flow |
|||
Viscosity | 1.00e+6 cP @Shear Rate 1.00 1/s, Temperature 230 °C |
1.00e+6 cP @Shear Rate 1.00 1/s, Temperature 446 °F |
|
DSM Arnite® TV4 441 (PBT+PET)-GF20 20% Glass Reinforced |
|||
Viscosity | 1.00e+6 cP @Shear Rate 0.100 1/s, Temperature 260 °C |
1.00e+6 cP @Shear Rate 0.100 1/s, Temperature 500 °F |
|
DSM Novamid® 2620A PA6/6T Extrusion |
|||
Viscosity | 1.00e+6 cP @Shear Rate 36.0 1/s, Temperature 305 °C |
1.00e+6 cP @Shear Rate 36.0 1/s, Temperature 581 °F |
ISO 11443 |
DuPont Performance Polymers Rynite® 408 NC010 PET Rynite® 408 NC010 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness, and temperature resistance.Inf.. |
|||
Viscosity | 1.00e+6 cP @Shear Rate 0.100 1/s, Temperature 260 °C |
1.00e+6 cP @Shear Rate 0.100 1/s, Temperature 500 °F |
|
DSM Novamid® 2620J PA6/6T Extrusion |