Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 6.9 cSt | 6.9 cSt | Base Oil; ASTM D445 |
Nye Lubricants 401 (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.9 cSt | 6.9 cSt | Base Oil; ASTM D445 |
Nye Lubricants 541(NF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.9 cSt | 6.9 cSt | Base Oil; ASTM D445 |
Nye Lubricants NPE-UC7 Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.9 cSt | 6.9 cSt | ASTM D445 |
ExxonMobil 427 Mobilmet 400 Series Mobilmet 400 Series products are high-performance multi-purpose cutting oils. They are chlorine-free, non-staining and non-corrosive. They are designed for light to moderate duty cutting operation.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.9 cSt | 6.9 cSt | ASTM D445 |
ExxonMobil Medium Mobil DTE Oil Named Series The Mobil DTE Oil Named Series of lubricants are premium performance circulating lubricants designed for applications including steam and hydro turbine sets and other systems where long lubricant se.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.9 cSt | 6.9 cSt | ASTM D445 |
ExxonMobil Univis N 32 UNIVIS N hydraulic oils are high-performance anti-wear fluids designed to meet the needs of all major manufacturers and users of hydraulic equipment. They feature high viscosity indexes (VIs), obtai.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.9 cSt | 6.9 cSt | |
ChevronTexaco Cepheus® 68 Texaco Cepheus oil deliver value throughThe ability to retain lubrication properties in the presence of water.Good rust protection from a carefully designed additive package.The ease with which they.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.9 cSt | 6.9 cSt | ASTM D445 |
ExxonMobil 427 Mobilmet 400 Series Mobilmet 400 Series products are high-performance multi-purpose cutting oils. They are chlorine-free, non-staining and non-corrosive. They are designed for light to moderate duty cutting operation.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.9 cSt | 6.9 cSt | ASTM D445 |
ExxonMobil Medium Mobil DTE Oil Named Series The Mobil DTE Oil Named Series of lubricants are premium performance circulating lubricants designed for applications including steam and hydro turbine sets and other systems where long lubricant se.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.9 cSt | 6.9 cSt | ASTM D445 |
ExxonMobil Univis N 32 UNIVIS N hydraulic oils are high-performance anti-wear fluids designed to meet the needs of all major manufacturers and users of hydraulic equipment. They feature high viscosity indexes (VIs), obtai.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.9 cSt | 6.9 cSt | |
ConocoPhillips Hydroclear® 250 Industrial Oil Description: Conoco Hydroclear Industrial Oil is a high-quality, general-purpose industrial lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Industrial Oil is recommende.. |