Polymer Property : Kinematic Viscosity at 100°C (212°F) = 19.3 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 100°C (212°F) 19.3 cSt
19.3 cSt
ChevronTexaco Quenchtex® MM
Texaco Quenchtex oils deliver value through:Controlled cooling of metals — Combines the high initial quenching speed of water with slow final quenching speed of oil.Safety — High flash point and f..
Kinematic Viscosity at 100°C (212°F) 19.3 cSt
19.3 cSt
ASTM D445
ChevronTexaco RPM® SAE 50 Heavy Duty Motor Oil
Features: Chevron RPM Heavy Duty Motor Oils are premium quality, mixed fleet motor oils meeting the performance requirements of all four-stroke gasoline engines and all naturally aspirated, turbocha..