Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Kinematic Viscosity at 100°C (212°F) = 12.3 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 100°C (212°F) 12.3 cSt
12.3 cSt
ASTM D445
ChevronTexaco ECO® SAE 30 Heavy Duty Motor Oil
Features:Chevron ECO Heavy Duty Motor Oils are formulated to be environmentally responsible engine lubricants. They use the highest quality re-refined base oils and specially selected additives desi..
Kinematic Viscosity at 100°C (212°F) 12.3 cSt
12.3 cSt
ASTM D445
ChevronTexaco ISO 150 Marine Oil E
FeaturesChevron Marine Oils E are formulated using a blend of high grade, medium viscosity index base oils and carefully balanced additive package to meet the crankcase need of marine steam engines...
Kinematic Viscosity at 100°C (212°F) 12.3 cSt
12.3 cSt
ASTM D445
ChevronTexaco ParaMount™ 6005 Paraffinic Process Oil
FeaturesChevron’s ParaMount Paraffinic Process Oils are highly saturated paraffinic process oils with very good color and low aromatic content.Chevron’s modern all-hydroprocessing technology assur..
Kinematic Viscosity at 100°C (212°F) 12.3 cSt
12.3 cSt
ASTM D445
ChevronTexaco Thread Sealing Compound
FeaturesChevron Thread Sealing Compound is a time-tested aluminum complex grease designed especially for casing and tubing connections in high-pressure oil well service, or wherever unusually severe..
Kinematic Viscosity at 100°C (212°F) 12.3 cSt
12.3 cSt
ASTM D445
ChevronTexaco NLGI 2 SRI Grease
FeaturesChevron SRI Grease is a high temperature ball and roller bearing grease.It is formulated with ISOSYN® base stocks, a synthetic polyurea ashless organic thickener, and high performance rust ..
Kinematic Viscosity at 100°C (212°F) 12.3 cSt
12.3 cSt
ConocoPhillips Hydroclear® 100 Rock Oil
Description: Conoco Hydroclear Rock Drill Oil is a high-quality, heavy-duty, extreme-pressure pneumatic tool lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Rock Drill ..
Copyright © lookpolymers.com All Rights Reserved