Polymer Property : Kinematic Viscosity at 40°C (104°F) = 64.6 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 64.6 cSt
64.6 cSt
ChevronTexaco 68 AW Hydraulic Oil
Texaco AW Hydraulic Oils deliver value through:High oxidation stability — Longer service life than with conventional lubricants in high pressure service.Rust and corrosion protection — Gives excel..
Kinematic Viscosity at 40°C (104°F) 64.6 cSt
64.6 cSt
ChevronTexaco 68 Way Lubricant
Texaco Way Lubricants deliver value through:Excellent separation from metalworking coolants — The SKC (SKC Gleittechnik) coolant separation test showed excellent separation from a wide variety of c..
Kinematic Viscosity at 40°C (104°F) 64.6 cSt
64.6 cSt
ChevronTexaco Alcaid® 60
Texaco Alcaid® oils deliver value through:Low pour points that permit oils to remain fluid at subzero temperatures.Ready separation from water, an important property where severe moisture condition..
Kinematic Viscosity at 40°C (104°F) 64.6 cSt
64.6 cSt
ChevronTexaco Capella® P 68
Texaco Capella P 68 delivers value through:Reduced oil carryover — Low volatility and greater ammonia immiscibility result in significantly less oil reaching the evaporator, increasing refrigeratio..
Kinematic Viscosity at 40°C (104°F) 64.6 cSt
64.6 cSt
ChevronTexaco Cepheus® 68
Texaco Cepheus oil deliver value throughThe ability to retain lubrication properties in the presence of water.Good rust protection from a carefully designed additive package.The ease with which they..
Kinematic Viscosity at 40°C (104°F) 64.6 cSt
64.6 cSt
ASTM D445
ChevronTexaco FM ISO 68 Lubricating Oil
Chevron Lubricating Oils FM are premium performance industrial lubricants designed for use in the food processing and other sensitive industries where incidental food contact may occur. Chevron Lubr..
Kinematic Viscosity at 40°C (104°F) 64.6 cSt
64.6 cSt
ASTM D445
ChevronTexaco Gear Compounds EP, ISO 68
FeaturesChevron Gear Compounds EP are multipurpose gear lubricants.They provide good thermal stability, extreme pressure protection, antiwear and demulsibility, oxidation, rust, corrosion control an..
Kinematic Viscosity at 40°C (104°F) 64.6 cSt
64.6 cSt
ASTM D445
ChevronTexaco HiPerSYN™ ISO 68 Oil
FeaturesChevron HiPerSYN Oils are synthetic compressor, bearing, and gear oils.They provide outstanding thermal and oxidation stability, high viscosity index, high flash point, low pour point, and e..
Kinematic Viscosity at 40°C (104°F) 64.6 cSt
64.6 cSt
ASTM D445
ChevronTexaco ISO 68 AIO
FeaturesChevron AIO (Chevron Authentic Industrial Oils) provide rust protection, oxidation inhibition, and foam suppression.Chevron AIO are good quality lubricants for any application not requiring ..
Kinematic Viscosity at 40°C (104°F) 64.6 cSt
64.6 cSt
ASTM D445
ChevronTexaco ISO 68 Ammonia Refrigeration Oil
FeaturesChevron Ammonia Refrigeration Oil provides superior wear protection for reciprocating, vane, and screw compressors.Chevron Ammonia Refrigeration Oil, formulated with ISOSYN® base stocks, is..
Kinematic Viscosity at 40°C (104°F) 64.6 cSt
64.6 cSt
ASTM D445
ChevronTexaco ISO 68 Hydraulic Oil AW
FeaturesChevron Hydraulic Oils AW are designed to give excellent hydraulic pump protection. They are formulated with refined paraffinic base oils. They provide excellent antiwear protection, oxidati..
Kinematic Viscosity at 40°C (104°F) 64.6 cSt
64.6 cSt
ASTM D445
ChevronTexaco ISO 68 Ultra Gear Lubricant
FeaturesChevron Ultra Gear Lubricants are premium grade, multipurpose gear lubricants.They are formulated with a unique extreme pressure additive using an inorganic borate compound. ISO 68, 150, 220..
Kinematic Viscosity at 40°C (104°F) 64.6 cSt
64.6 cSt
ASTM D445
ChevronTexaco ISO 68 Utility Oil HVI
FeaturesChevron Utility Oil HVI is a high quality, high viscosity index uncompounded oil with excellent water separating characteristics.Chevron Utility Oil HVI possesses good natural thermal and ox..
Kinematic Viscosity at 40°C (104°F) 64.6 cSt
64.6 cSt
ASTM D445
ChevronTexaco ISO 68 Utility Oil LVI
FeaturesChevron Utility Oils LVI are general purpose lubricants. Chevron Utility Oils LVI are light-colored oils that possess excellent natural low pour points, along with low carbon-forming tendenc..
Kinematic Viscosity at 40°C (104°F) 64.6 cSt
64.6 cSt
ASTM D445
ChevronTexaco Mechanism LPS® ISO 68 Hydraulic Oil
Chevron Mechanism LPS Hydraulic Oils are highly refined, paraffinic oils containing oxidation and rust inhibitors, and special antiwear additives to extend the life of hydraulic pumps and motor part..
Kinematic Viscosity at 40°C (104°F) 64.6 cSt
64.6 cSt
ChevronTexaco Meropa® 68
Texaco Meropa oils deliver value through:Gear set efficiencies — High thermal stability EP system maintains clean gear and bearing surfaces, minimizing deposits which interfere with effective lubri..
Kinematic Viscosity at 40°C (104°F) 64.6 cSt
64.6 cSt
ChevronTexaco Pinnacle® 68
Texaco Pinnacle oils deliver value through:Long lubricant life in high temperature operations — The synthetic hydrocarbon base oils and proprietary additive package used in these products provide o..
Kinematic Viscosity at 40°C (104°F) 64.6 cSt
64.6 cSt
ChevronTexaco Rando® HD 68
Texaco Rando HD oils deliver value through:Longer equipment life — Special antiwear additive package reduces wear by protecting surfaces when load causes breakdown of the lubricant film.Reduced dow..
Kinematic Viscosity at 40°C (104°F) 64.6 cSt
64.6 cSt
ChevronTexaco Rando® HD 68 Ashless
Texaco Rando HD Ashless oils deliver value through:Premium performance — Ashless formulation meets or exceeds pump manufacturer requirements for viscosity, rust and corrosion protection, hydrolytic..
Kinematic Viscosity at 40°C (104°F) 64.6 cSt
64.6 cSt
ASTM D445
ChevronTexaco Regal® 68 R&O
Texaco Regal R&O oils deliver value through:Prolonged oil service life — Excellent oxidation stability provided by the multi-component inhibitor system resists oil breakdown during exposure to high..
Kinematic Viscosity at 40°C (104°F) 64.6 cSt
64.6 cSt
ASTM D445
ChevronTexaco Regal® N-68 R&O
Texaco Regal R&O oils deliver value through:Prolonged oil service life — Excellent oxidation stability provided by the multi-component inhibitor system resists oil breakdown during exposure to high..
Kinematic Viscosity at 40°C (104°F) 64.6 cSt
64.6 cSt
ASTM D445
ChevronTexaco Rykon® ISO 68 Oil AW
FeaturesChevron Rykon Oils AW are designed to give maximum hydraulic pump protection.Chevron Rykon Oils AW are formulated with ISOSYN® base stocks.They provide excellent antiwear protection, oxidat..
Kinematic Viscosity at 40°C (104°F) 64.6 cSt
64.6 cSt
ASTM D445
ChevronTexaco TEGRA® ISO 68 Synthetic Compressor Oil
FeaturesChevron Tegra Synthetic Compressor Oils are synthetic compressor lubricants formulated with the highest quality polyalphaolefin (PAO) base fluids.They provide excellent thermal and oxidation..
Kinematic Viscosity at 40°C (104°F) 64.6 cSt
64.6 cSt
ASTM D445
ChevronTexaco Vistac® ISO 68 Way Oil
FeaturesChevron Way Oils Vistac provide extreme pressure and antiwear protection and have stringiness and oiliness characteristics. As indicated by part of the name, Vistac, these lubricants have an..
Kinematic Viscosity at 40°C (104°F) 64.6 cSt
64.6 cSt
ChevronTexaco Canopus® 68
Texaco Canopus oils deliver value through:High resistance to forming emulsions due to excellent water separating characteristics.Long lubricant life provided by outstanding stability.Good lubricant ..
Kinematic Viscosity at 40°C (104°F) 64.6 cSt
64.6 cSt
ASTM D445
ChevronTexaco Clarity® ISO 68 Hydraulic Oil AW
FeaturesChevron Clarity Hydraulic Oils AW are designed to give maximum protection to hydraulic pumps in highperformance industrial applications as well as in environmentally sensitive areas.They are..
Kinematic Viscosity at 40°C (104°F) 64.6 cSt
64.6 cSt
ChevronTexaco Cygnus® 68 Hydraulic Oil
Texaco Cygnus Hydraulic Oils deliver value through:High quality control — Enables customer to use lubricants almost as pure as the food being processedHigh performance — Provides lubrication bette..
Kinematic Viscosity at 40°C (104°F) 64.6 cSt
64.6 cSt
ASTM D445
ChevronTexaco GST® ISO 68 Oil
FeaturesChevron GST Oils are designed to meet the critical demands of:gas, steam, and hydroelectric turbine bearing lubricationreduction gear lubrication in marine operationsThey are an excellent re..
Kinematic Viscosity at 40°C (104°F) 64.6 cSt
64.6 cSt
ASTM D445
ChevronTexaco Vistac® ISO 68 Way Oil D
FeaturesChevron Way Oils Vistac D are high quality lubricants designed to meet the critical lubrication demands for the slides and ways of machine tools.Chevron Way Oils Vistac D is formulated with ..
Kinematic Viscosity at 40°C (104°F) 64.6 cSt
64.6 cSt
ASTM D445
ChevronTexaco Cetus® PAO 68
Texaco Cetus PAO oils deliver value through:Long lubricant life in high temperature operations — Outstanding thermal and oxidation stability.Extended machinery life and increased compressor efficie..