Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 5950 cSt | 5950 cSt | |
ChevronTexaco Sugartex® Heavy Texaco Sugartex delivers value through:Reliability — High lubricant film strength withstands heavy shock loads and provides protection under boundary lubrication to minimize wear rate and prevent f.. |