Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 345 cSt | 345 cSt | ASTM D445 |
Solvay Specialty Polymers FOMBLIN® YR PFPE Lubricant FOMBLIN YR perfluoropolyether fluids have excellent high temperature stability, good low temperature properties, very good E.P. and wear characteristics, good evaporative loss, and good viscosity in.. |