Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 147 cSt | 147 cSt | |
Lubriplate SYNAC 150 Diester-Based Synthetic Air Compressor Fluid These diester-based synthetic air compressor fluids are outstanding for applications where the fluid is subjected to high temperature and high stress conditions over extended drain intervals.Synac S.. |
|||
Kinematic Viscosity at 40°C (104°F) | 147 cSt | 147 cSt | ASTM D445 |
Solvay Specialty Polymers FOMBLIN® Y45 PFPE Lubricant FOMBLIN Y perfluoropolyether fluids have the following unique features; excellent high temperature stability; good low temperature properties; very good E.P. and wear characteristics; good evaporati.. |