Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 135 cSt | 135 cSt | |
Lubriplate 130-A Calcium Type Multi-Purpose Grease These water resistant calcium type greases are designed for plain bearings, cams, slides, and other light-duty applications where temperatures do not exceed 170°F. See special applications. Appli.. |
|||
Kinematic Viscosity at 40°C (104°F) | 135 cSt | 135 cSt | |
Lubriplate 130-AA Calcium Type Multi-Purpose Grease These water resistant calcium type greases are designed for plain bearings, cams, slides, and other light-duty applications where temperatures do not exceed 170°F. See special applications. Appli.. |
|||
Kinematic Viscosity at 40°C (104°F) | 135 cSt | 135 cSt | |
Lubriplate 630-2 Lithium Based Multi-Purpose Grease These popular lithium type greases are excellent for a wide range of lubrication demands thus reducing the need to carry large grease inventories. They show exceptional resistance to water, steam, a.. |
|||
Kinematic Viscosity at 40°C (104°F) | 135 cSt | 135 cSt | |
Lubriplate 630-A Lithium Based Multi-Purpose Grease These popular lithium type greases are excellent for a wide range of lubrication demands thus reducing the need to carry large grease inventories. They show exceptional resistance to water, steam, a.. |
|||
Kinematic Viscosity at 40°C (104°F) | 135 cSt | 135 cSt | |
Lubriplate 630-AA Lithium Based Multi-Purpose Grease These popular lithium type greases are excellent for a wide range of lubrication demands thus reducing the need to carry large grease inventories. They show exceptional resistance to water, steam, a.. |
|||
Kinematic Viscosity at 40°C (104°F) | 135 cSt | 135 cSt | |
Lubriplate 930-2 Bentone Type Multi-Purpose Grease Formulated for higher temperature applications. They are shear stable, multi-purpose greases for both plain and anti-friction bearings. This series works well up to 375°F / 191°C and for short.. |
|||
Kinematic Viscosity at 40°C (104°F) | 135 cSt | 135 cSt | |
Lubriplate 930-A Bentone Type Multi-Purpose Grease Formulated for higher temperature applications. They are shear stable, multi-purpose greases for both plain and anti-friction bearings. This series works well up to 375°F / 191°C and for short.. |
|||
Kinematic Viscosity at 40°C (104°F) | 135 cSt | 135 cSt | |
Lubriplate 930-AA Bentone Type Multi-Purpose Grease Formulated for higher temperature applications. They are shear stable, multi-purpose greases for both plain and anti-friction bearings. This series works well up to 375°F / 191°C and for short.. |
|||
Kinematic Viscosity at 40°C (104°F) | 135 cSt | 135 cSt | |
Lubriplate AC-3 Petroleum-Based Air Compressor Fluid Formulated to reduce carbon & varnish buildup. They contain fluid zinc to effectively fight friction & wear thus reducing heat & foaming. Available in six ISO grades.AC Series Air Compressor Oils ar.. |
|||
Kinematic Viscosity at 40°C (104°F) | 135 cSt | 135 cSt | |
Lubriplate H0-3 Petroleum-Based Heavy-Duty Hydraulic Oil Formulated for superior performance, this series contains fluid zinc to effectively reduce ring & vane wear. Excellent anti-rust, anti-corrosion, anti-foam and anti-oxidation properties. High anilin.. |
|||
Kinematic Viscosity at 40°C (104°F) | 135 cSt | 135 cSt | |
Lubriplate SPO-244 Petroleum-Based Gear, Bearing, & Recirculating Oil Petroleum-based oils specifically designed for industrial applications such as gear cases, bearings, chains, machine ways, and general oiling. These tacky lubricants will provide anti-wear lubricati.. |