Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 750 SUS
750 SUS
Lubriplate 130-A Calcium Type Multi-Purpose Grease
These water resistant calcium type greases are designed for plain bearings, cams, slides, and other light-duty applications where temperatures do not exceed 170°F. See special applications. Appli..
Saybolt Viscosity at 100°F 750 SUS
750 SUS
Lubriplate 130-AA Calcium Type Multi-Purpose Grease
These water resistant calcium type greases are designed for plain bearings, cams, slides, and other light-duty applications where temperatures do not exceed 170°F. See special applications. Appli..
Saybolt Viscosity at 100°F 750 SUS
750 SUS
Lubriplate 630-2 Lithium Based Multi-Purpose Grease
These popular lithium type greases are excellent for a wide range of lubrication demands thus reducing the need to carry large grease inventories. They show exceptional resistance to water, steam, a..
Saybolt Viscosity at 100°F 750 SUS
750 SUS
Lubriplate 630-A Lithium Based Multi-Purpose Grease
These popular lithium type greases are excellent for a wide range of lubrication demands thus reducing the need to carry large grease inventories. They show exceptional resistance to water, steam, a..
Saybolt Viscosity at 100°F 750 SUS
750 SUS
Lubriplate 630-AA Lithium Based Multi-Purpose Grease
These popular lithium type greases are excellent for a wide range of lubrication demands thus reducing the need to carry large grease inventories. They show exceptional resistance to water, steam, a..
Saybolt Viscosity at 100°F 750 SUS
750 SUS
Lubriplate 72-C Oil Food Machinery Oil
Class H-2** oil, for use as a steam peeler oil as it provides an oiliness film which prevents chatter.Available in Bottles, Jugs, Pails, 1/4 Drums and DrumsH-1 Class Lubricants are manufactured with..
Saybolt Viscosity at 100°F 750 SUS
750 SUS
Lubriplate 930-2 Bentone Type Multi-Purpose Grease
Formulated for higher temperature applications. They are shear stable, multi-purpose greases for both plain and anti-friction bearings. This series works well up to 375°F / 191°C and for short..
Saybolt Viscosity at 100°F 750 SUS
750 SUS
Lubriplate 930-A Bentone Type Multi-Purpose Grease
Formulated for higher temperature applications. They are shear stable, multi-purpose greases for both plain and anti-friction bearings. This series works well up to 375°F / 191°C and for short..
Saybolt Viscosity at 100°F 750 SUS
750 SUS
Lubriplate 930-AA Bentone Type Multi-Purpose Grease
Formulated for higher temperature applications. They are shear stable, multi-purpose greases for both plain and anti-friction bearings. This series works well up to 375°F / 191°C and for short..
Saybolt Viscosity at 100°F 750 SUS
750 SUS
Lubriplate FML 0 Anhydrous Calcium USP Mineral Oil-Based Food Machinery Grade Grease
These white, multi-purpose greases have been popular in the food processing industry for years. Available in three NLGI densities for a wide variety of applications.FML Series greases are available ..
Saybolt Viscosity at 100°F 750 SUS
750 SUS
Lubriplate FML 1 Anhydrous Calcium USP Mineral Oil-Based Food Machinery Grade Grease
These white, multi-purpose greases have been popular in the food processing industry for years. Available in three NLGI densities for a wide variety of applications.FML Series greases are available ..
Saybolt Viscosity at 100°F 750 SUS
750 SUS
Lubriplate FML 2 Anhydrous Calcium USP Mineral Oil-Based Food Machinery Grade Grease
These white, multi-purpose greases have been popular in the food processing industry for years. Available in three NLGI densities for a wide variety of applications.FML Series greases are available ..