Physical Properties Metric English Comments
Specific Gravity 8.00 g/cc
8.00 g/cc
Lucas-Milhaupt Silvaloy® 0 Brazing Alloy
Silvaloy 0 is used for the brazing of copper and copper alloys, brass and bronze. It can also be used on silver, tungsten and molybdenum. It is primarily used for the joining of copper-to-copper on ..
Specific Gravity 8.00 g/cc
8.00 g/cc
Lucas-Milhaupt Silvaloy® 2 Brazing Alloy
Silvaloy 2 is used for the brazing of copper and copper alloys, brass and bronze. It can also be used on silver, tungsten and molybdenum. It is primarily used for the joining of copper-to-copper on ..
Specific Gravity 8.00 g/cc
8.00 g/cc
Ecomass® 1002ZD93 Tungsten Filled COPA
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsHigh Specific GravityTungsten Powder Filled Co-Polyamide (COPA)Excellent ToughnessInformation provided by ..
Specific Gravity 8.00 g/cc
8.00 g/cc
ASTM D792
Ecomass® 1080ZD92 Tungsten Powder Filled Polyamide Alloy, Injection Molding Grade
High Specific Gravity, Tungsten Powder Filled Polyamide (PA) Alloy, Excellent Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing..
Specific Gravity 8.00 g/cc
8.00 g/cc
ASTM D792
Clariant Renol PA2SP0009HW Nylon 6, Heavyweight Compound
Data provided by Clariant Masterbatches
Copyright © lookpolymers.com All Rights Reserved