Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 3.67 g/cc | 3.67 g/cc | Mixed |
Tra-Con Tra-Duct 2921 Silver-Filled Adhesive Information provided by Tra-Con Inc. |
|||
Specific Gravity | 3.67 g/cc | 3.67 g/cc | Mixed |
Tra-Con Tra-Duct 2929 Room Temperature Conductive Flexible Silver Epoxy Adhesive TRA-DUCT 2929 is recommended for electronic bonding, coating and sealing applications that require high flexibility coupled with excellent electrical and mechanical properties. This two-part epoxy a.. |