Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 3.10 g/cc | 3.10 g/cc | |
Parker Chomerics CHO-SHIELD® 2003 Conductive Coating Electrically conductive coatings provide corrosion protection for enclosure flanges which mate with EMI shielding gaskets. They can also provide a corrosion resistant conductive surface coating on a.. |
|||
Specific Gravity | 3.10 g/cc | 3.10 g/cc | |
Parker Chomerics Tecknit® 0002 Highly Conductive Adhesive-Sealant Silver Silicone Description: TECKNIT® 0002 is a pure silver filled, one component RTV silicone adhesive-sealant. It is ready to use without mixing and cures quickly at room temperature on exposure to moisture in .. |
|||
Specific Gravity | 3.10 g/cc | 3.10 g/cc | Part A |
Epoxy Technology EPO-TEK® E4110 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® E4110 is an electrically conductive, silver-filled epoxy paste. This two component system is designed for low temperature curing from ambient to 80°C, although other.. |
|||
Specific Gravity | 3.10 g/cc | 3.10 g/cc | |
Parker Chomerics CHO-SHIELD® 2001 Conductive Coating Electrically conductive coatings provide corrosion protection for enclosure flanges which mate with EMI shielding gaskets. They can also provide a corrosion resistant conductive surface coating on a.. |
|||
Specific Gravity | 3.10 g/cc | 3.10 g/cc | |
Parker Chomerics CHO-SHIELD® 2002 Conductive Coating Electrically conductive coatings provide corrosion protection for enclosure flanges which mate with EMI shielding gaskets. They can also provide a corrosion resistant conductive surface coating on a.. |