Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 3.01 g/cc @Temperature 25.0 °C |
3.01 g/cc @Temperature 77.0 °F |
|
Dow Corning SE 4447 CV KIT Two-part liquid silicone elastomer designed for applications requiring very high thermal conductivity and electrical insulation.Information provided by Dow Corning |