Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.60 - 2.10 g/cc | 1.60 - 2.10 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL 1285R Reinforced Conductive Elastomer Seal These materials are fabric-reinforced, silver-plated-aluminum filled EMI seals for airframe shielding applications. These seal materials can also be used to maintain surface electrical continuity at.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group 2572 AMC Glass fiber reinforced Polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, good abrasion stability, high flame retardance in combin.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group 3505 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group 3535 Epoxy Glass fiber-reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties adn dimensional stability even at high temperatures. Form: Low dust granulate pack.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group RALUPOL® 4385 UP Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very high arc resistance, very high mechanical values. This product meets the allowed upper limits for heavy.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group RALUPOL® 4802 UP Polyester Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group RALUPOL® 4806 UP Glass-fiber reinforced polyester molding compound. Very low mold shrinkage and post-shrinkage, very good mechanical strength, very good electrical values, better performance values compared to UP 80.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group RALUPOL® 802 UP Polyester Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength, good heat resistance. This product meets the allowed up.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group RALUPOL® 804 UP Polyester Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy m.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group RALUPOL® 8601 UP Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic moulding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical stren.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group RALUPOL® 8602 UP Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic molding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical streng.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group SURAPLAST 54 UPA Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group SURAPLAST UPA 63 UP Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ASTM D792 |
Mar-Bal MB1000-PC Thermoset Polyester Composite Molding Compound A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro.. |
|||
Specific Gravity | 2.00 - 2.10 g/cc | 2.00 - 2.10 g/cc | ASTM D792 |
Mar-Bal MB2000-8 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Specific Gravity | 2.06 - 2.10 g/cc | 2.06 - 2.10 g/cc | ASTM D792 |
Adamas Adalon® 118 PTFE, 23/2% Carbon/Graphite Filled Information provided by Adamas, HPM |
|||
Specific Gravity | 1.70 - 2.10 g/cc | 1.70 - 2.10 g/cc | |
Bulk Molding Compounds BMC 1000 Thermoset Polyester, Food Grade BMC 1000 is a general purpose, food contact grade, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. As with all other BMC, Inc. compounds, .. |
|||
Specific Gravity | 1.60 - 2.10 g/cc | 1.60 - 2.10 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL® 6502 Conductive Elastomer Description: Highest performance in harsh environments; excellent shielding; best choice for corrosion requirements against aluminum.Molded and ExtrudedRoHS CompliantInformation provided by Chomeric.. |
|||
Specific Gravity | 2.03 - 2.10 g/cc | 2.03 - 2.10 g/cc | ASTM D792 |
Technetics Group Texolon™ 8534 PTFE
(Unverified Data**) PTFE CharacteristicsChemical ResistanceThermal StabilityCryogenic PropertiesLow Coefficient of FrictionLow Surface EnergyLow Dielectric ConstantHigh Volume and Surface ResistivityFlame ResistanceApp.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group 5567 DAP Diallyl Phthalate (DAP), Cast, Mineral Filler Glass-fiber reinforced diallyl phthalate molding compound free from halogens. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exc.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group RALUPOL® 8605 UP Polyester Glass fiber reinforced polyester molding compound. Resistant to hydrolysis. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU dire.. |