Polymer Property : Specific Gravity = 1.88 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.88 g/cc
1.88 g/cc
Omya OMYAFLOW® F - SY Calcium Carbonate
A high purity, fine, wet ground natural calcium carbonate available in slurry form.Applications: Decorative paints.Information supplied by Omya North America.
Specific Gravity 1.88 g/cc
1.88 g/cc
Park Electrochemical Nelcote® P-650R Polyester Prepreg, 7781 E-Glass Reinforced
Nelcote® P-650R is a non-styrenated/low VOC polyester resin system that has been designed for optical clarity. P-650 exhibits good mechanical properties up to 250°F.Key Features and Benefits:Non-s..
Specific Gravity 1.88 g/cc
1.88 g/cc
ASTM D792
PolyOne Edgetek® SF-35GF-25MN/000 Polyphenylene Sulfide (PPS), Glass/Mineral Filled  (discontinued **)
Description/Features:Glass/Mineral ReinforcedUL 94 V0 (HEM TEST)PolyOne First ChoiceInformation provided by PolyOne Corporation.
Specific Gravity 1.88 g/cc
1.88 g/cc
ISO 1183
Lehmann & Voss LUVOCOM® 1301-7508 PPS, linear, with glass spheres
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic..
Specific Gravity 1.88 g/cc
1.88 g/cc
ASTM D297
Greene Tweed CHEMRAZ® 522 Perfluoroelastomer
Chemraz®, a proprietary Greene, Tweed compound, has the broadest chemical resistance of any elastomeric material. Chemraz combines the resilience and sealing force of an elastomer with chemical r..
Specific Gravity 1.88 g/cc
1.88 g/cc
ASTM 792
Multibase Multi-Flex® D 2010 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good F..
Specific Gravity 1.88 g/cc
1.88 g/cc
ASTM D297, 15
Seals Eastern 7040 Fluorocarbon-Elastomer
Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type..
Specific Gravity 1.88 g/cc
1.88 g/cc
ASTM D297, 15
Seals Eastern 5795 Fluorocarbon-Elastomer
Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type..
Specific Gravity 1.88 g/cc
1.88 g/cc
BYK Cloisite® 93A Nanoclay
Cloisite® 93A is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.Information provided by Southern Clay ProductsSouthern Clay Pr..
Specific Gravity 1.88 g/cc
1.88 g/cc
3M Dyneon™ FPO 3740 Fluoroelastomer
3M™ Dyneon™ FPO 3740 is a peroxide curable fluoroelastomer terpolymer containing 69.5 wt% fluorine. FPO 3740 can be used in compression, transfer or injection molding, and extrusion processes. Fea..
Specific Gravity 1.88 g/cc
1.88 g/cc
ASTM D792
Cheng Yu Plastic E2350 Flame Retardant PET, 50% Glass Fiber
Specific Gravity 1.88 - 1.94 g/cc
1.88 - 1.94 g/cc
Bulk Molding Compounds BMC 1454 for Injection Molding Circuit Breakers
BMC 1454 is a special low-cost material developed specifically for injection molding circuit breakers. It has considerable flame, arc and track resistance. BMC 1454 is a medium strength material wit..
Specific Gravity 1.88 - 1.96 g/cc
1.88 - 1.96 g/cc
Bulk Molding Compounds BMC 605LS Mineral Filled, Glass Fiber Reinforced Polyester Compound
BMC 605LS molding compound is a low-shrink, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is characterized by good mol..
Specific Gravity 1.88 - 1.92 g/cc
1.88 - 1.92 g/cc
Bulk Molding Compounds BMC 610 - SP Mineral Filled, Glass Reinforced Polyester Compound, with UV Stabilizer
BMC 610 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is set a part form other medium impact el..
Specific Gravity 1.88 - 1.92 g/cc
1.88 - 1.92 g/cc
molded
Bulk Molding Compounds BMC 610 Mineral filled, glass-fiber-reinforced polyester compound
BMC 610 molding compound is a mineral filled, glass­ fiber­ reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is set a part form other medium impact..
Specific Gravity 1.88 g/cc
1.88 g/cc
Bulk Molding Compounds BMC 615 Mineral Filled, Glass Fiber Reinforced Polyester Compound
BMC 615 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ext..
Specific Gravity 1.88 g/cc
1.88 g/cc
ASTM D792
PolyOne Edgetek® SF-35GF-25MN/000 L Polyphenylene Sulfide (PPS), Glass/Mineral Filled  (discontinued **)
Description/Features:Glass/Mineral ReinforcedPTFE LubricatedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.