Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.86 g/cc | 1.86 g/cc | |
P & P Technology Silver/Aluminum Conductive Adhesive P & P Technology conductive silver/aluminum adhesive is a one part electrically conductive room temperature curing elastomer. It is supplied as a readily extrudable paste that cures rapidly when exp.. |
|||
Specific Gravity | 1.86 g/cc | 1.86 g/cc | ASTM D792 |
Premix Premi-Glas® 8105 Glass Reinforced Polyester BMC
(discontinued **) Description: Premi-Glas® 8105 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits: Ex.. |
|||
Specific Gravity | 1.86 g/cc | 1.86 g/cc | ASTM D792 |
Samsung Cheil Industries Infino® XP-2165BM PPS Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.86 g/cc | 1.86 g/cc | ASTM D792 |
Samsung Cheil Industries Infino® XP-2165BM PPS Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.86 g/cc | 1.86 g/cc | |
Silberline Silvex® 620-25-D Silvex® D grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited for use .. |
|||
Specific Gravity | 1.86 g/cc | 1.86 g/cc | |
Silberline Sparkle Silver Ultraâ„¢ 6605 Sparkle Silver Ultraâ„¢ grades are very bright lenticular automotive aluminum pigments. They offer a very smooth patina and narrow particle size distribution, allowing the formulator to create ve.. |
|||
Specific Gravity | 1.86 g/cc | 1.86 g/cc | |
Silberline Sparkle Silver® Premier 55 Sparkle Silver® Premier flakes provide more uniform surfaces than Sparkle Silver® products, and also sharper edges and controlled particle size distribution. "Sparkle Silver® Premier or Sil.. |
|||
Specific Gravity | 1.86 g/cc | 1.86 g/cc | Part A |
Epoxy Technology EPO-TEK® T7109-18 Electrically Insulating Epoxy Paste Material Description: A flexible, electrically insulating epoxy paste designed for low stress and heat dissipation applications. Alternative to EPO-TEK® T7109-17.Information Provided by Epoxy Tec.. |
|||
Specific Gravity | 1.86 g/cc | 1.86 g/cc | |
3M Dyneon™ FT 2320 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FT 2320 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul.. |
|||
Specific Gravity | 1.86 g/cc | 1.86 g/cc | |
3M Dyneon™ FT 2350 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FT 2350 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul.. |
|||
Specific Gravity | 1.86 g/cc | 1.86 g/cc | |
3M Dyneon™ FT 2430 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FT 2430 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul.. |
|||
Specific Gravity | 1.86 g/cc | 1.86 g/cc | |
3M Dyneon™ FT 2481 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FT 2481 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul.. |
|||
Specific Gravity | 1.86 g/cc | 1.86 g/cc | |
3M Dyneon™ FX 11818 Fluoroelastomer 3M™ Dyneon™ Flouroelastomer FX 11818 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formu.. |
|||
Specific Gravity | 1.86 g/cc | 1.86 g/cc | |
3M Dyneon™ LTFE 6400Z Low Temperature Fluoroelastomer 3M™ Dyneon™ Low Temperature Fluoroelastomers LTFE 6400Z are technically advanced low temperature, peroxide-cured fluoroelastomers, designated as a FKM type 3 elastomer per ASTM D1418. They are des.. |
|||
Specific Gravity | 1.86 g/cc | 1.86 g/cc | |
3M Dyneon™ LTFE 6400ZC Low Temperature Fluoroelastomer 3M™ Dyneon™ Low Temperature Fluoroelastomers LTFE 6400ZC are technically advanced low temperature, peroxide-cured fluoroelastomers, designated as a FKM type 3 elastomer per ASTM D1418. They are de.. |
|||
Specific Gravity | 1.86 g/cc | 1.86 g/cc | |
Bulk Molding Compounds BMC 2270 Mineral Filled, Glass Reinforced Polyester BMC 2270 molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression and transfer molding. It is a general purpose material with medium impact strength a.. |
|||
Specific Gravity | 1.86 g/cc | 1.86 g/cc | |
Bulk Molding Compounds BMC 620M Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 620M molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, and stuffer injection molding It is characterized by high impact strength, good mol.. |