Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.85 - 1.90 g/cc | 1.85 - 1.90 g/cc | |
Premix Premi-Glas® 2207-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2207-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Specific Gravity | 1.85 - 1.95 g/cc | 1.85 - 1.95 g/cc | |
Premix Premi-Ject® 1102H Fiberglass Reinforced Thermoset BMC Premi-Ject® 1102H is a fiberglass reinforced thermoset bulk molding compound for coil encapsulation applications.Key features and benefits are:Designed with unique flow properties to encapsulate co.. |
|||
Specific Gravity | 1.85 - 2.35 g/cc | 1.85 - 2.35 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL® 6370 Conductive Elastomer Flame Retardant Conductive Silicone Elastomer. CHO-SEAL 6370 EMI gaskets are conductive elastomers engineered for use in commercial electronic equipment where a high degree of flame retardancy and c.. |
|||
Specific Gravity | 1.85 - 1.95 g/cc | 1.85 - 1.95 g/cc | ISO 1183 |
Raschig Group EPOXIDUR® 3585 EP Epoxy, Molded, Glass Fiber Filler Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures, excel.. |
|||
Specific Gravity | 1.85 - 1.95 g/cc | 1.85 - 1.95 g/cc | ISO 1183 |
Raschig Group RESINOL® 87120 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | |
Industrial Laminates/Norplex NP841 Glass Fabric
(discontinued **) Description: Woven glass fabric with phenolic resin. Contains Kocite® for controlled conductivity. Acts as static electricity drain to protect electrical and electronic equipment.Thickness Tested: .. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | |
Garlock Viton® 501 Fluoroelastomer Sheet Rubber Style #501 sheet rubber, made with VITON® fluoroelastomer, is a high-performance product resistant to heat, oils, fuels, numerous acids and other chemicals.Information provided by Garlock Rubber .. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | |
Industrial Laminates/Norplex MC514MG Glass Fabric Description: MC514MG is made with a woven glass fabric in combination with high temperature, conductive, phenolic resin system.NP514MG has excellent flexural, compressive and impact strengths at roo.. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | ASTM 792 |
Multibase Multi-Flex® G 7155 TPE Styrene Ethylene Butylene Styrene Block Copolymer Features: Chemical Resistance, Good Noise DampingOzone Resistant Thermal Stability, Good Forms:PelletsProcessing Method:Injection MoldingBlow MoldingExtrusion Uses: Automotive ApplicationsInforma.. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | ASTM D-792 |
Glastic SG-200 Corner Angles Corner angles used for coil winding.Information provided by Glastic Corporation |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Isotropic CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Unidirectional CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | at 25°C |
Daikin DAI-EL G-702 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: General purpose with excellent elongation and tear strength.Informatio.. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | at 25°C |
Daikin DAI-EL G-704 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Information provided by Daikin Industries. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | at 25°C |
Daikin DAI-EL G-716 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Minimal compression set and fast vulcanization.Information provided by.. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | at 25°C |
Daikin DAI-EL G-723 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Excellent mold releasability, non-sticking.Information provided by Dai.. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | at 25°C |
Daikin DAI-EL G-751 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: General purpose with excellent metal bonding and compression set.Infor.. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | at 25°C |
Daikin DAI-EL G-752 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Information provided by Daikin Industries. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | at 25°C |
Daikin DAI-EL G-755 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Extrusion of hose and tubing, etc.Information provided by Daikin Indus.. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | at 25°C |
Daikin DAI-EL G-763 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Excellent mold releasability for O-rings.Information provided by Daiki.. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | at 25°C |
Daikin DAI-EL G-781 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Information provided by Daikin Industries. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | at 25°C |
Daikin DAI-EL G-783 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Fast vulcanization, for complex shapes.Information provided by Daikin .. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | |
3M Dyneon™ FLS 2530 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FLS 2530 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formu.. |
|||
Specific Gravity | 1.85 - 1.95 g/cc | 1.85 - 1.95 g/cc | |
Bulk Molding Compounds BMC 100 Thermoset Polyester, GP BMC 100 is a high strength, low shrink general purpose molding compound. It can be supplied in bulk or extruded in pre-weighted slugs. Due to the excellent flow and controlled reactivity, BMC 100 is.. |
|||
Specific Gravity | 1.85 - 1.95 g/cc | 1.85 - 1.95 g/cc | |
Bulk Molding Compounds BMC 200 Thermoset Polyester, Electrical Grade BMC 200 is a high strength, low shrink molding compound. It can be supplied in bulk or extruded in pre-weighted slugs.Typical applications are circuit breakers, insulators, bobbins, electrical conne.. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | |
Bulk Molding Compounds BMC 6605A Polyester Molding Compound |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | Silicone Property; Arlon SQA-TMS-024 |
Arlon Thermabond® 99A90N008 Primerless Electronic Adhesive
(discontinued **) Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer. |
|||
Specific Gravity | 1.85 - 1.95 g/cc | 1.85 - 1.95 g/cc | ISO 1183 |
Raschig Group RESINOL® 400 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |