Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.85 - 1.90 g/cc | 1.85 - 1.90 g/cc | |
Premix Premi-Glas® 2207-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2207-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Specific Gravity | 1.85 - 1.95 g/cc | 1.85 - 1.95 g/cc | |
Premix Premi-Ject® 1102H Fiberglass Reinforced Thermoset BMC Premi-Ject® 1102H is a fiberglass reinforced thermoset bulk molding compound for coil encapsulation applications.Key features and benefits are:Designed with unique flow properties to encapsulate co.. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | |
Premix Thermoplastics PRESEAL® TPE 6080 General Description:PRESEAL® TPE 6080 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasket applications. It can also be used as conductors or in grounding.. |
|||
Specific Gravity | 1.85 - 2.35 g/cc | 1.85 - 2.35 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL 6370 Conductive Elastomer Commercial Grade Conductive Elastomer Extrusions. These materials offer excellent cost/performance characteristics for commercial EMI gasket applications. These silicone and fluorosilicone based con.. |
|||
Specific Gravity | 1.85 - 2.35 g/cc | 1.85 - 2.35 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL® 6370 Conductive Elastomer Flame Retardant Conductive Silicone Elastomer. CHO-SEAL 6370 EMI gaskets are conductive elastomers engineered for use in commercial electronic equipment where a high degree of flame retardancy and c.. |
|||
Specific Gravity | 1.85 - 2.35 g/cc | 1.85 - 2.35 g/cc | ASTM D792 |
Parker Chomerics Tecknit Consil®-E 815 Extruded Silver-Filled Silicone Elastomer Description: CONSIL-E is a continuously extruded silicone elastomer filled with silver-plated inert particles. It is a medium hardness material providing high electrical conductivity and moisture se.. |
|||
Specific Gravity | 1.85 - 1.95 g/cc | 1.85 - 1.95 g/cc | ISO 1183 |
Raschig Group EPOXIDUR® 3581 S ZC EP Epoxy Molding Compound Inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very good sealing connection on .. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | Arlon SQA-TMS-024 |
Arlon Thermabond® R37340X008 Primerless Electronic Adhesive
(discontinued **) Liner: 1 mil FEP; Product: uncured Silicone Rubber; Carrier: 3 mil PTFE coated fiberglas |
|||
Specific Gravity | 1.85 - 1.95 g/cc | 1.85 - 1.95 g/cc | ISO 1183 |
Raschig Group RESINOL® 87120 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | |
Premix Premi-Glas® 1200-50VE 1200-50 VE SMC
(discontinued **) Description: Premi-Glas® 1200-50 VE is a sheet molding compound.Market: StructuralInformation provided by Premix. |
|||
Specific Gravity | 1.85 - 1.95 g/cc | 1.85 - 1.95 g/cc | ASTM D792 |
Mar-Bal MB3000-15NY Thermoset Polyester Composite Molding Compound A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | |
Garlock Viton® 501 Fluoroelastomer Sheet Rubber Style #501 sheet rubber, made with VITON® fluoroelastomer, is a high-performance product resistant to heat, oils, fuels, numerous acids and other chemicals.Information provided by Garlock Rubber .. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | ASTM D-792 |
Glastic GLASTHERM HT220 Insulation Sheet Glastherm Grade HT220 is a thermal insulation sheet that is a highly heat-resistant material that combines low thermal conductivity with very high compressive strength at molding temperature. It is.. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | |
Industrial Laminates/Norplex MC514MG Glass Fabric Description: MC514MG is made with a woven glass fabric in combination with high temperature, conductive, phenolic resin system.NP514MG has excellent flexural, compressive and impact strengths at roo.. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | ASTM 792 |
Multibase Multi-Flex® G 7150 TPE Styrene Ethylene Butylene Styrene Block Copolymer Features: Chemical Resistance, Good Noise DampingOzone Resistant Thermal Stability, Good Forms:PelletsProcessing Method:Injection MoldingBlow MoldingExtrusion Uses: Automotive ApplicationsInforma.. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | |
Shinil Chemical SHINCON PES Electro Conductive Polymer SHINCON is the product line of SHINIL's electrically conductive compound which is able to dissipate the electrostatic charge (ESD) effectively. Shinil has developed SHINCON products using Shinil's .. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Isotropic CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | at 25°C |
Daikin DAI-EL G-702 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: General purpose with excellent elongation and tear strength.Informatio.. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | at 25°C |
Daikin DAI-EL G-704 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Information provided by Daikin Industries. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | at 25°C |
Daikin DAI-EL G-716 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Minimal compression set and fast vulcanization.Information provided by.. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | at 25°C |
Daikin DAI-EL G-723 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Excellent mold releasability, non-sticking.Information provided by Dai.. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | at 25°C |
Daikin DAI-EL G-752 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Information provided by Daikin Industries. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | at 25°C |
Daikin DAI-EL G-755 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Extrusion of hose and tubing, etc.Information provided by Daikin Indus.. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | at 25°C |
Daikin DAI-EL G-763 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Excellent mold releasability for O-rings.Information provided by Daiki.. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | at 25°C |
Daikin DAI-EL G-781 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Information provided by Daikin Industries. |
|||
Specific Gravity | 1.85 - 1.95 g/cc | 1.85 - 1.95 g/cc | |
Bulk Molding Compounds BMC 350 Thermoset Polyester, Medium Impact BMC 350 is a cosmetic and appliance grade material with excellent heat and stain resistant properties. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk.Typical ap.. |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | |
Bulk Molding Compounds BMC 6605A Polyester Molding Compound |
|||
Specific Gravity | 1.85 g/cc | 1.85 g/cc | Silicone Property; Arlon SQA-TMS-024 |
Arlon Thermabond® 99A90N008 Primerless Electronic Adhesive
(discontinued **) Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer. |