Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.71 g/cc | 1.71 g/cc | ASTM D792 |
PolyOne OnForce™ LFT UR-60 LGF/000 Natural Polyurethane, Unspecified (PUR, Unspecified) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Specific Gravity | 1.71 g/cc | 1.71 g/cc | ASTM D792 |
Polymer Resources NY66-G60 Nylon 66, 60% Glass Reinforced Nylon 66, 60% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test.. |
|||
Specific Gravity | 1.71 g/cc | 1.71 g/cc | ASTM D-792 |
PlastiComp Complet® LGF60 - TPU Rigid Thermoplastic Polyurethane, 60% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 60% long glass fiber reinforcementInformation provided by Plas.. |
|||
Specific Gravity | 1.71 g/cc | 1.71 g/cc | |
Lord Adhesives Thermosetâ„¢ ME-531 Underfill Encapsulant LORD Thermosetâ„¢ ME-531 encapsulant is a high purity, semiconductor grade epoxy underfill product developed for the encapsulation of flip chip devices. It is formulated to reduce warpage and wit.. |
|||
Specific Gravity | 1.71 g/cc | 1.71 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105-7583 PEEK, with glass fiber and PTFE, improved wear resistance Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Good friction and wear behaviour especially at increased temperatures.Chemical and hydroly.. |
|||
Specific Gravity | 1.71 g/cc | 1.71 g/cc | |
Silberline EX 2629 Stabilized UV EX 2629 provides a medium-fine particle size grade of acid resistant aluminum flake pigment for use in one pack UV cured coatings. The aluminum flake is stabilized to increase the shelf life of the .. |
|||
Specific Gravity | 1.71 g/cc | 1.71 g/cc | |
Silberline EX 2871 Stabilized UV EX 2871 provides a non-leafing, fine particle size grade of aluminum flake pigment for use in one pack UV cured coatings. The aluminum flake is stabilized to increase the shelf life of the product i.. |
|||
Specific Gravity | 1.71 g/cc | 1.71 g/cc | |
Silberline Sparkle Silver® 3130-AR Sparkle Silver® 3130-AR is a coarse, non-leafing, acid stain resistant aluminum flake pigment with greater hiding power than the related Sparkle Silver® 3122-AR. It is characterized by high sp.. |
|||
Specific Gravity | 1.71 g/cc | 1.71 g/cc | ASTM D792 |
Lubrizol ISOPLAST™ 2560 Engineering Thermoplastic Polyurethane Resin for Medical Applications Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaAvailableInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Specific Gravity | 1.71 g/cc | 1.71 g/cc | ASTM D1505 |
DuPont™ Tedlar® TWH20BS3 Satin White Polyvinyl Fluoride Film Properties of DuPont™ Tedlar® polyvinyl fluoride (PVF) biaxially oriented film include excellent resistance to weathering, outstanding mechanical properties, and inertness towards a wide variety o.. |
|||
Specific Gravity | 1.71 g/cc | 1.71 g/cc | |
Bulk Molding Compounds BMC 680 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 680 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression and stuffer injection molding It is characterized by good moldability, very high impa.. |
|||
Specific Gravity | 1.71 g/cc | 1.71 g/cc | ASTM D792 |
E-Polymers SEPAZ® LA60 PA66 LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Specific Gravity | 1.71 g/cc | 1.71 g/cc | ASTM D792 |
E-Polymers SEPAZ® LB60 PA6 LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Specific Gravity | 1.71 g/cc | 1.71 g/cc | ASTM D792 |
E-Polymers SEPAZ® C140GP 40% Glass Fiber Reinforced LCP Resin Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding .. |