Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.59 g/cc | 1.59 g/cc | ASTM D792 |
Nylene® 7250 C HS , 50% Glass Fiber/Ceramic Reinforced, Low Warp, High Stiffness Specialty Nylon Description: Nylene® 7250 C HS is a 50% glass fiber/ceramic reinforced, low warp, high stiffness specialty nylon. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are al.. |
|||
Specific Gravity | 1.59 g/cc | 1.59 g/cc | ASTM D792 |
Ovation Polymers Opnyl OP6GF50 Nylon 6, 50% Glass Reinforced, Dry Nylon 6 - Glass reinforced (50 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. For Nylon compounds the m.. |
|||
Specific Gravity | 1.59 g/cc | 1.59 g/cc | ASTM D792 |
Quadrant EPP Ketron® CM GF30 Compression Molded, 30% Glass Reinforces Polyethererther Ketone(ASTM Product Data Sheet) |
|||
Specific Gravity | 1.59 g/cc | 1.59 g/cc | ASTM D792 |
PolyOne Edgetek® ES-30GF/000 Black Polyethersulfone (PESU) Edgetek™ ES-30GF/000 Black XP120031Information provided by PolyOne |
|||
Specific Gravity | 1.59 g/cc | 1.59 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105-7776 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Low warpage, isotropic shrinkage characteristics.Emergency running pro.. |
|||
Specific Gravity | 1.59 g/cc | 1.59 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1301-7153 PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. .. |
|||
Specific Gravity | 1.59 g/cc | 1.59 g/cc | ASTM D792 |
LG Chemical LUCEL GB-325 Low Warpage POM, 25% Glass Bead Filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Specific Gravity | 1.59 g/cc | 1.59 g/cc | ASTM D792 |
Kolon KOCETAL® GF305 G/F Reinforced Acetal Resin Glass fiber reinforced, improved stiffness. Applications: Products for high stiffness, improved fatigue properties. Information provided by API-Kolon. |
|||
Specific Gravity | 1.59 g/cc | 1.59 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1/GF/40/TF/13 Polyamide 66, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Specific Gravity | 1.59 g/cc | 1.59 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP PFL38S PA 6 LNP* LUBRICOMP* PFL38S is a compound based on Nylon 6 resin containing 40% Glass Fiber, 15% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant |
|||
Specific Gravity | 1.59 g/cc | 1.59 g/cc | ASTM D792 |
SABIC Innovative Plastics Valox® 553 PBT+PC 30% GR PBT+PC, UL94 V-0. Reduced warpage characteristics.Applications; appliance handles, spotlights, electric motors, pump housings, etc. |
|||
Specific Gravity | 1.59 g/cc | 1.59 g/cc | ASTM D792 |
Samyang Tribit® 1500GN30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant Characteristics:G/F reinforcedFlame retardantHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A.. |
|||
Specific Gravity | 1.59 g/cc | 1.59 g/cc | ASTM D792 |
Samyang Tribit® 1551GN30 PBT, Impact Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1551GN30 is an impact grade.Information pro.. |
|||
Specific Gravity | 1.59 g/cc | 1.59 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP VERTON MV00ES PP LNP* VERTON* MV00ES is primarily a concentrate used for blending purposes. This is a 70% long glass fiber Polypropylene compound. Added features of this grade are: Heat Stabilized |
|||
Specific Gravity | 1.59 g/cc | 1.59 g/cc | ASTM D297, 15 |
Seals Eastern 7182A Fluorocarbon-Elastomer Formulated AFLAS® high-temperature, high-pressure "sour" oil & gas service. Resistant to extrusion. Excellent acid and base resistance.Information provided by Seals Eastern, Inc. |
|||
Specific Gravity | 1.59 g/cc | 1.59 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP VERTON RV00AE PA 66 LNP* VERTON* RV00AE is a compound based on Nylon 66 containing 50% Long Glass Fiber. Added features of this grade include: Easy Molding, Structural. |
|||
Specific Gravity | 1.59 g/cc | 1.59 g/cc | ASTM D792 |
Teknor Apex Fireguard® 910-A10-NL2 Polyvinyl Chloride, Flexible Notes: RoHS Compliant Features: Flame Retardant; Low Smoke Emission Wire Types: CL2P; CL3P; CMP; FPLP; MPP; OFNP Agency Ratings: NEC Article 725; NEC Article 760; NEC Article 770; NEC Article 800;.. |
|||
Specific Gravity | 1.59 g/cc | 1.59 g/cc | ASTM D792 |
A. Schulman PAPERMATCH® T-4776/50 Specialty Masterbatch DescriptionPAPERMATCH® T-4776/50 is a specialty masterbatch formulated to impart paper-like properties to polyolefin films. PAPERMATCH® T-4776/50 is a white, medium opacity grade designed to prov.. |
|||
Specific Gravity | 1.59 g/cc | 1.59 g/cc | ASTM D792 |
A. Schulman PAPERMATCH® T-4776/50 Specialty Masterbatch DescriptionPAPERMATCH® T-4776/50 is a specialty masterbatch formulated to impart paper-like properties to polyolefin films. PAPERMATCH® T-4776/50 is a white, medium opacity grade designed to prov.. |
|||
Specific Gravity | 1.59 g/cc | 1.59 g/cc | ASTM D792 |
Colorite Polymers CS7559LS Wire and Cable Insulation Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Specific Gravity | 1.59 g/cc | 1.59 g/cc | |
Aremco Pyro-Paint™ 634-AS High Temperature Refractory Coating This alumina-silica based advanced coating is rated for continuous service temperatures up to 2300 °F. Provides excellent adhesion to ceramic fiber blankets, modules and boards and resists wetting .. |
|||
Specific Gravity | 1.59 - 1.63 g/cc | 1.59 - 1.63 g/cc | ASTM D-792 |
Axiall 2400F Plenum Flexible PVC Plenum-grade optical fiber buffer compound. UL QMTM2 recognized component for plenum cable compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.59 g/cc | 1.59 g/cc | Laminate; ASTM D792 |
Azdel AZMET® CM20350 35% continuous random fiber mat / PBT resin matrix AZDEL® CM20350 is a glass mat thermoplastic laminate based upon a random oriented continuous fiber mat contained within a Polybutylene Terephthalate (PBT) resin matrix. This composite material fea.. |
|||
Specific Gravity | 1.59 g/cc | 1.59 g/cc | |
Aremco Glass-Coat™ SGC4000 High Temperature Specialty Coatings Silicone-Glass Silicone-glass-ceramic, gray, low viscosity, scratch resistant coating for stainless steel to 900°F (482°C) |
|||
Specific Gravity | 1.59 g/cc | 1.59 g/cc | Method A; ASTM D792 |
LNP Thermocomp® JF-1006 EM Polyethersulfone, Glass Fiber Reinforcement
(discontinued **) Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st.. |
|||
Specific Gravity | 1.59 g/cc | 1.59 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL APS440 PPE+PPS (Asia Pacific) |