Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.52 - 1.58 g/cc
1.52 - 1.58 g/cc
ASTM D792
PTS PBT-20GFR 20% Glass Filled
PBT, injection molding grade, 20% glass fiber reinforced, flame retardant, exceptional flowability and processability, colorable.Information provided by PTS LLC.
Specific Gravity 0.980 - 1.58 g/cc
0.980 - 1.58 g/cc
ASTM D792
Parker Chomerics CHO-SEAL® 0860 Conductive Elastomer
Description: Low-end shielding and ESD protection; high tensile strength; no corrosion or fluid resistance.Extruded onlyRoHS CompliantInformation provided by Chomerics
Specific Gravity 1.52 - 1.58 g/cc
1.52 - 1.58 g/cc
NBR NM-IEC 60811-1-3
Karina 70911-35/1-HY-AC Ivory PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.52 - 1.58 g/cc
1.52 - 1.58 g/cc
ASTM D 792
Karina 813-35/1-DY-SN-ERYB Compound PVC Ivory
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.52 - 1.58 g/cc
1.52 - 1.58 g/cc
ASTM D 792
Karina 837-10/119-E-ERYB White PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.52 - 1.58 g/cc
1.52 - 1.58 g/cc
ASTM D 792
Karina 837-35/1-E-ERYB Ivory PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.52 - 1.58 g/cc
1.52 - 1.58 g/cc
ASTM D 792
Karina E 48/1-IE Black Color Concentrate MBU
Carbon black concentrate recommended for application in polyolefins and polyolefinic and PVC compounds for general purposes. Recommended usage of 2% to 4%.Information provided by Karina Indústri..
Specific Gravity 1.54 - 1.58 g/cc
1.54 - 1.58 g/cc
ASTM D-792
Axiall 2460F Plenum Flexible PVC
Plenum-grade optical fiber jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.52 - 1.58 g/cc
1.52 - 1.58 g/cc
ASTM D792
BLUESTAR PBT 403M-G20 20% Glass Filled
PBT, injection molding grade, 20% glass fiber reinforced, flame retardant, exceptional flowability and processability, colorable.Information provided by Polymer Technology and Services, LLC (PTS).
Specific Gravity 1.54 - 1.58 g/cc
1.54 - 1.58 g/cc
ASTM D-792
Axiall 02520 Plenum Flexible PVC
Non-lead stabilized plenum grade jacket with good low temperature properties. Recommended for Category 5 applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2..