Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.51 - 1.57 g/cc | 1.51 - 1.57 g/cc | ASTM D 792 |
Karina E 32/76-FC-LMP Orange Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.53 - 1.57 g/cc | 1.53 - 1.57 g/cc | ASTM D-792 |
Axiall 1063-119i Coax & Telecom Flexible PVC Highly flame retardant CMR jacket for use over HDPE inners in 20-22 mil wall applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.53 - 1.57 g/cc | 1.53 - 1.57 g/cc | ASTM D-792 |
Axiall 01561 Plenum Flexible PVC Non-lead stabilized CAT 5 plenum jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |