Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.479 - 1.921 g/cc | 1.479 - 1.921 g/cc | ASTM D792 |
Parker Chomerics Tecknit Consil®-V 751 Extruded Silver-Filled Silicone Elastomer Description: Consil-V is an extruded silicone elastomer filled with silver-plated inert particles. The V-shape cross section is ideally suited for applications requiring low closure force gasketing... |
|||
Specific Gravity | 1.479 - 2.001 g/cc | 1.479 - 2.001 g/cc | |
Parker Chomerics Tecknit Teckfip™ FIP-X Formed in Place Conductive Elastomer Description: FIP-X is Tecknit’s newest compound and features a conductive powder that is a unique particle combining tungsten carbide and aluminum. The premium advantage of this compound is its ab.. |