Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.153 g/cc | 1.153 g/cc | |
Dow SPECTRIM™ 35A Isocyanate SPECTRIM™ 35A reaction moldable polymer is one component (SPECTRIM™ 35B-S is the other) of a two-component polyurethane system that incorporates advanced internal mold release (IMR) technology dev.. |
|||
Specific Gravity | 1.153 g/cc | 1.153 g/cc | |
Dow SPECTRIM™ 50A Isocyanate SPECTRIM™ 50A reaction moldable polymer is one component (SPECTRIM™ 35A is the other) of a two-component polyurethane system that incorporates advanced internal mold release (IMR) technology devel.. |