Polymer Property : Specific Gravity = 0.992 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 0.992 g/cc
0.992 g/cc
ASTM D792
Polymax® Maxelast® A9855A TPE, ABS/PC Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform..
Specific Gravity 0.992 g/cc
0.992 g/cc
ASTM D792
Polymax® Maxelast® N8855 TPE, Nylon Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Auto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInformation from Alliance Polymers & Se..
Specific Gravity 0.992 g/cc
0.992 g/cc
ASTM D792
Polymax® Maxelast® N8860 TPE, Nylon Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Auto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInformation from Alliance Polymers & Se..
Specific Gravity 0.992 g/cc
0.992 g/cc
ASTM D792
Polymax® Maxelast® N8960 TPE, Nylon Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Auto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInformation from Alliance Polymers & Se..
Specific Gravity 0.992 g/cc
0.992 g/cc
ASTM D792
Polymax® Maxelast® P1970 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Specific Gravity 0.992 g/cc
0.992 g/cc
ASTM D792
Polymax® Maxelast® P2880 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Specific Gravity 0.992 g/cc
0.992 g/cc
ASTM D792
Polymax® Maxelast® P3850 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Specific Gravity 0.992 g/cc
0.992 g/cc
ASTM D792
Polymax® Maxelast® P3862 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Specific Gravity 0.992 g/cc
0.992 g/cc
ASTM D792
Polymax® Maxelast® P3865B TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Specific Gravity 0.992 g/cc
0.992 g/cc
ASTM D792
Teknor Apex Telcar® TL-86-K975-A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..