Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.981 - 0.987 g/cc | 0.981 - 0.987 g/cc | |
LG Chemical LGflex GL300 Plasticizer Features: Excellent Viscosity, Heat Stability and Non-endocrine disrupterApplication: PVC Calenderings/Leathers, Sheets, Gloves, HoseInformation provided by LG Chemical |