Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.978 - 0.984 g/cc @Temperature 25.0 °C |
0.978 - 0.984 g/cc @Temperature 77.0 °F |
ASTM D4052 |
PolyOne reFlex™ 300 Plasticizer, Bio-derived Bio-derived, non-phthalate plasticizer; USDA BioPreferred® certified 99% biobased.Information provided by PolyOne |
|||
Specific Gravity | 0.978 - 0.984 g/cc @Temperature 25.0 °C |
0.978 - 0.984 g/cc @Temperature 77.0 °F |
ASTM D4052 |
PolyOne Synplast™ DOP-N Di (2-ethylhexyl) Phthalate Branched C8 phthalate esterInformation provided by PolyOne |
|||
Specific Gravity | 0.978 - 0.984 g/cc @Temperature 25.0 °C |
0.978 - 0.984 g/cc @Temperature 77.0 °F |
ASTM D4052 |
PolyOne Synplast™ NOTM-E Tri (n-octyl) Trimellitate Linear trimellitate esterContains 0.10-0.15 wt% 1,1,3-Tris (2-methyl-4hydroxy-5-t-butyl phenyl) butane antioxidantInformation provided by PolyOne |
|||
Specific Gravity | 0.978 - 0.984 g/cc @Temperature 25.0 °C |
0.978 - 0.984 g/cc @Temperature 77.0 °F |
ASTM D4052 |
PolyOne Synplast™ NOTM-PPC Tri (n-octyl) Trimellitate CPSIA HR 4040 Compliant Linear trimellitate esterContains 0.10-0.15 wt% 1,1,3-Tris (2-methyl-4hydroxy-5-t-butyl phenyl) butane antioxidantInformation provided by PolyOne |