Polymer Property : Specific Gravity = 0.984 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 0.978 - 0.984 g/cc

@Temperature 25.0 °C
0.978 - 0.984 g/cc

@Temperature 77.0 °F
ASTM D4052
PolyOne reFlex™ 300 Plasticizer, Bio-derived
Bio-derived, non-phthalate plasticizer; USDA BioPreferred® certified 99% biobased.Information provided by PolyOne
Specific Gravity 0.978 - 0.984 g/cc

@Temperature 25.0 °C
0.978 - 0.984 g/cc

@Temperature 77.0 °F
ASTM D4052
PolyOne Synplast™ DOP-N Di (2-ethylhexyl) Phthalate
Branched C8 phthalate esterInformation provided by PolyOne
Specific Gravity 0.978 - 0.984 g/cc

@Temperature 25.0 °C
0.978 - 0.984 g/cc

@Temperature 77.0 °F
ASTM D4052
PolyOne Synplast™ NOTM-E Tri (n-octyl) Trimellitate
Linear trimellitate esterContains 0.10-0.15 wt% 1,1,3-Tris (2-methyl-4hydroxy-5-t-butyl phenyl) butane antioxidantInformation provided by PolyOne
Specific Gravity 0.978 - 0.984 g/cc

@Temperature 25.0 °C
0.978 - 0.984 g/cc

@Temperature 77.0 °F
ASTM D4052
PolyOne Synplast™ NOTM-PPC Tri (n-octyl) Trimellitate
CPSIA HR 4040 Compliant Linear trimellitate esterContains 0.10-0.15 wt% 1,1,3-Tris (2-methyl-4hydroxy-5-t-butyl phenyl) butane antioxidantInformation provided by PolyOne