Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.972 g/cc | 0.972 g/cc | ASTM 792 |
Multibase Nylex™ 2185 HFX Natural Polyamide + PP Forms: PelletsProcessing Methods:Injection moldingFeatures:Tensile Strength, HighInformation provided by Multibase |
|||
Specific Gravity | 0.972 g/cc | 0.972 g/cc | ASTM D792 |
Polymax® Maxelast® A9810 TPE, ABS/PC Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform.. |
|||
Specific Gravity | 0.972 g/cc | 0.972 g/cc | ASTM D792 |
Polymax® Maxelast® A9830 TPE, ABS/PC Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform.. |
|||
Specific Gravity | 0.972 g/cc | 0.972 g/cc | ASTM D792 |
Polymax® Maxelast® P2855B TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.972 g/cc | 0.972 g/cc | ASTM D792 |
Polymax® Maxelast® P3675 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.972 g/cc | 0.972 g/cc | ASTM D792 |
Polymax® Maxelast® P3838 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.972 g/cc | 0.972 g/cc | ASTM D792 |
Polymax® Maxelast® P3845H TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.972 g/cc | 0.972 g/cc | ASTM D792 |
Polymax® Maxelast® P3855 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.972 g/cc | 0.972 g/cc | ASTM D792 |
Polymax® Maxelast® P3860 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.972 g/cc | 0.972 g/cc | ASTM D792 |
Polymax® Maxelast® P3865A TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.972 g/cc | 0.972 g/cc | ASTM D792 |
Polymax® Maxelast® P3899 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.972 g/cc | 0.972 g/cc | ASTM D792 |
Polymax® Maxelast® P3960 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.972 g/cc | 0.972 g/cc | ASTM D792 |
Network Polymers Softflex® 0470 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Specific Gravity | 0.972 g/cc | 0.972 g/cc | ASTM 792 |
Multibase Multi-Flex® A 9402 AH Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Specific Gravity | 0.972 - 0.977 g/cc @Temperature 20.0 °C |
0.972 - 0.977 g/cc @Temperature 68.0 °F |
DIN 51 757/ASTM D4052 |
The Chemical Company VESTINOL® 9 Diisononyl Phthalate, C6H4(COOC9H19)2 Diisononyl Phthalate (DINP) C6H4(COOC9H19)2, is a clear, colorless, and almost odorless liquid chemical. It is soluble in most organic solvents. DINP is primarily used as a PVC plasticizer. As compa.. |
|||
Specific Gravity | 0.972 g/cc @Temperature 25.0 °C |
0.972 g/cc @Temperature 77.0 °F |
|
Dow Corning XIAMETER® PMCPOHX-4000 Polymer 2000CS Is chemically equivalent to DOW CORNING® 3-0133 POLYMER 2,000 CS. Polydimethylsiloxane polymer with terminated, curable silanol functionality, viscosity 2,000 cp.Information provided by Dow Corning.. |
|||
Specific Gravity | 0.972 g/cc @Temperature 25.0 °C |
0.972 g/cc @Temperature 77.0 °F |
|
Dow Corning 360 Medical Fluid, 1000 CST. Colorless and odorless polydimethysiloxane fluid for lubrication and siliconization of glass, metals, plastics and rubber in medical applications.Information provided by Dow Corning |
|||
Specific Gravity | 0.972 g/cc @Temperature 25.0 °C |
0.972 g/cc @Temperature 77.0 °F |
|
Dow Corning 360 Medical Fluid, 12,500 CST. Colorless and odorless polydimethysiloxane fluid for lubrication and siliconization of glass, metals, plastics and rubber in medical applications.Information provided by Dow Corning |