Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.934 g/cc | 0.934 g/cc | ISO 1183 |
Polimeri Europa Flexirene® FH 56 A Butene Copolymer Linear Low Density Polyethylene Flexirene FH 56 A is a butene copolymer with medium density (C4-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films manufactured with Flexirene FH 56 A are characte.. |
|||
Specific Gravity | 0.934 g/cc | 0.934 g/cc | ISO 1183 |
Polimeri Europa Clearflex® FF 508 Octene Copolymer Linear Medium Density Polyethylene Clearflex FF 508 is an octene copolymer linear medium density polyethylene (C8-LMDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films manufactured with Clearflex FF 50.. |
|||
Specific Gravity | 0.934 g/cc | 0.934 g/cc | 20/20°C |
LyondellBasell TPNB Tripropylene glycol normal butyl ether Information provided by Lyondell. |
|||
Specific Gravity | 0.934 g/cc | 0.934 g/cc | ISO 1183 |
Total MDPE HF 513 Medium Density Polyethylene, Blown Film MDPE HF 513 is a medium density polyethylene produced by slurry loop low pressure process with hexene as co-monomer.MDPE HF 513 is a semi-high molecular weight polyethylene giving excellent mechanic.. |
|||
Specific Gravity | 0.934 g/cc | 0.934 g/cc | ASTM D792 |
Total Lumicene® mPE M 3410 EP Metallocene Medium Density Film Resin
(Unverified Data**) Polyethylene: Metallocene Medium Density Film ResinCharacteristics:Outstanding clarity and glossExcellent bubble stabilityHigh StiffnessGood puncture resistanceGood tear strengthGood heat sealing p.. |
|||
Specific Gravity | 0.934 g/cc @Temperature 25.0 °C |
0.934 g/cc @Temperature 77.0 °F |
|
Dow Corning XIAMETER® PMCPPMX-200 10CS Silicone Fluid Is chemically equivalent to DOW CORNING® 200 FLUID 10CS. 100% active, 10 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning |
|||
Specific Gravity | 0.934 g/cc | 0.934 g/cc | ISO 1183 |
Total Lumicene® mPE M 3427 Metallocene Polyethylene, Cast Film Lumicene® mPE M 3427 is a second generation metallocene based Polyethylene with hexene as comonomer.Lumicene® mPE M 3427 can be processed at high output rates with low extrusion pressure, low neck.. |