Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.921 - 0.925 g/cc | 0.921 - 0.925 g/cc | ASTM D1505 |
LG Chemical SEETEC BF315 LDPE Characteristics: Good Processability and Excellent Optical PropertiesApplications: Masking filmCAS No. 9002-88-4Information provided by LG Chemical |
|||
Specific Gravity | 0.919 - 0.925 g/cc @Temperature 25.0 °C |
0.919 - 0.925 g/cc @Temperature 77.0 °F |
ASTM D4052 |
PolyOne Synplast™ DOA-FDA Di (2-ethylhexyl) Adipate Branched C8 adipate esterInformation provided by PolyOne |
|||
Specific Gravity | 0.919 - 0.925 g/cc @Temperature 25.0 °C |
0.919 - 0.925 g/cc @Temperature 77.0 °F |
ASTM D4052 |
PolyOne Synplast™ DOA-N Di (2-ethylhexyl) Adipate Branched C8 adipate esterInformation provided by PolyOne |