Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.923 g/cc | 0.923 g/cc | ISO 1183 |
Polimeri Europa Greenflex® FL 25 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FL 25 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FL 25 show good optical properties and excellent sealability.Main Applications: .. |
|||
Specific Gravity | 0.923 g/cc | 0.923 g/cc | ISO 1183 |
Polimeri Europa Riblene® FH 20 Low Density Polyethylene - Blown Film Extrusion Riblene FH 20 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FH 20 is characterized by a good balance between processability and mechanical properties.Films manufac.. |
|||
Specific Gravity | 0.923 g/cc | 0.923 g/cc | ISO 1183 |
Polimeri Europa Riblene® GM 30 Low Density Polyethylene - Coating Grade Riblene GM 30 is a medium fluidity low density polyethylene resin (LDPE).Main Applications: Riblene GM 30 is suitable for coating applications where low neck-in and high manufacturing speed are req.. |
|||
Specific Gravity | 0.923 g/cc | 0.923 g/cc | ISO 1183 |
Polimeri Europa Riblene® GM 30 R Low Density Polyethylene - Coating Grade Riblene GM 30 R is a medium fluidity low density polyethylene resin (LDPE).Main Applications: Riblene GM 30 R is suitable for coating applications where low neck-in and high manufacturing speed are.. |
|||
Specific Gravity | 0.923 g/cc | 0.923 g/cc | 20/20°C |
LyondellBasell PM Propylene glycol methyl ether Available in electronic grade.Information provided by Lyondell. |
|||
Specific Gravity | 0.923 g/cc | 0.923 g/cc | ASTM D1505 |
SCG Chemicals EL-Leneâ„¢ LD2305F Low Density Polyethylene Film Key Characteristics:Excellent clarity and glossGood zip formationContains 1000 ppm slip agent and 500 ppm antiblocking agentRecommended Applications:Zip bagsGeneral purpose film for food packagingIn.. |
|||
Specific Gravity | 0.923 g/cc | 0.923 g/cc | ASTM D792 |
A. Schulman CP851 High Flow, Injection Molding Grade DescriptionCP 851 is a high flow injection molding grade of conventional (high pressure) low density polyethylene. ApplicationCP 851 meets the specifications in FDA Regulation 21 CFR177.1520 (c)3.1.. |
|||
Specific Gravity | 0.923 g/cc | 0.923 g/cc | ASTM D792 |
Teknor Apex Uniprene® UN-7010-64NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin.. |
|||
Specific Gravity | 0.923 g/cc | 0.923 g/cc | ASTM D792 |
A. Schulman CP851 High Flow, Injection Molding Grade DescriptionCP 851 is a high flow injection molding grade of conventional (high pressure) low density polyethylene. ApplicationCP 851 meets the specifications in FDA Regulation 21 CFR177.1520 (c)3.1.. |
|||
Specific Gravity | 0.923 g/cc | 0.923 g/cc | ISO 1183 |
Total LDPE 1022 FH 24 Low Density Polyethylene - Blown Film LDPE 1022 FH 24 is a low density polyethylene made by a high pressure process.LDPE 1022 FH 24 is a slip and anti-block formulated grade.LDPE 1022 FH 24 is suited to many applications in the field of.. |
|||
Specific Gravity | 0.923 g/cc | 0.923 g/cc | ASTM D792 |
A. Schulman CP851 High Flow, Injection Molding Grade DescriptionCP 851 is a high flow injection molding grade of conventional (high pressure) low density polyethylene. ApplicationCP 851 meets the specifications in FDA Regulation 21 CFR177.1520 (c)3.1.. |
|||
Specific Gravity | 0.923 g/cc | 0.923 g/cc | ASTM D792 |
A. Schulman CP851 High Flow, Injection Molding Grade DescriptionCP 851 is a high flow injection molding grade of conventional (high pressure) low density polyethylene. ApplicationCP 851 meets the specifications in FDA Regulation 21 CFR177.1520 (c)3.1.. |
|||
Specific Gravity | 0.923 g/cc | 0.923 g/cc | ASTM D792 |
A. Schulman CP851 High Flow, Injection Molding Grade DescriptionCP 851 is a high flow injection molding grade of conventional (high pressure) low density polyethylene. ApplicationCP 851 meets the specifications in FDA Regulation 21 CFR177.1520 (c)3.1.. |
|||
Specific Gravity | 0.923 g/cc | 0.923 g/cc | ISO 1183 |
Total Lumicene® mPE M 2310 EP Metallocene Polyethylene, Blown Film Lumicene® mPE M 2310 EP is a second generation metallocene based Linear Low Density Polyethylene with hexene as comonomer.Lumicene® mPE M 2310 EP can be processed at high output rates with low ext.. |
|||
Specific Gravity | 0.923 g/cc | 0.923 g/cc | ASTM D792 |
A. Schulman CP851 High Flow, Injection Molding Grade DescriptionCP 851 is a high flow injection molding grade of conventional (high pressure) low density polyethylene. ApplicationCP 851 meets the specifications in FDA Regulation 21 CFR177.1520 (c)3.1.. |
|||
Specific Gravity | 0.923 g/cc | 0.923 g/cc | ASTM D1505 |
Chevron Phillips MarFlex® HHM TR-258 Low Density Linear Polyethylene, Blown Film This LDLPE is tailored for applications that require:Good processabilityGood melt strengthGood drawdownGood strengthSatin finishGood MD & TD shrinkageGood contact clarity and lower gel contentTypica.. |
|||
Specific Gravity | 0.923 g/cc | 0.923 g/cc | ASTM D1505/D792 |
Braskem EB853/72 Blown Film Extrusion Low Density Polyethylene Automatic packaging for several products; High transparency films.Additives: Antiblock, DInformation provided by Braskem. |
|||
Specific Gravity | 0.923 g/cc | 0.923 g/cc | ASTM D1505/D792 |
Braskem PB208 Injection Molding Low Density Polyethylene Injected lids and caps; Large flat surface injected pieces.Information provided by Braskem. |
|||
Specific Gravity | 0.923 g/cc | 0.923 g/cc | ASTM D1505/D792 |
Braskem EB853 Cast Film Extrusion Low Density Polyethylene LLDPE and HDPE blends.Information provided by Braskem. |
|||
Specific Gravity | 0.923 g/cc | 0.923 g/cc | ISO 1183 |
Total LDPE 1022 FN 24 Low Density Polyethylene - Blown Film LDPE 1022 FN 24 is a low density polyethylene made by a high pressure process without antioxidant.LDPE 1022 FN 24 is suited to many applications in the field of consumer, industrial, food or hygiene.. |
|||
Specific Gravity | 0.923 g/cc | 0.923 g/cc | ASTM D1505/D792 |
Braskem BF0323/12HC Blown Film Extrusion Low Density Polyethylene Shrink films; Automatic packaging of liquid products (FFS).Additives: Antiblock, DInformation provided by Braskem. |
|||
Specific Gravity | 0.923 g/cc | 0.923 g/cc | ASTM D1505/D792 |
Braskem F2523 Blown Film Extrusion Low Density Polyethylene Automatic packaging for several products; High transparency films.Additives: Antiblock, DInformation provided by Braskem. |
|||
Specific Gravity | 0.923 g/cc | 0.923 g/cc | ASTM D792 |
PolyOne Syncure™ System S100NA Polyethylene, Crosslinked (XLPE) Syncure™ systems are two part moisture crosslinkable compounds, UL bulletinized easy processing, high strength, colorable cable insulation compound suitable for service entrance cables. RoHS compli.. |
|||
Specific Gravity | 0.923 g/cc | 0.923 g/cc | ASTM D1505/D792 |
Braskem BF0323HC Blown Film Extrusion Low Density Polyethylene Heavy-duty bags; Agriculture, Coextruded and shrink films for pallets.Information provided by Braskem. |