Polymer Property : Specific Gravity = 0.922 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 0.922 g/cc
0.922 g/cc
ASTM D792
Polymax® Maxelast® A9735C TPE, ABS/PC Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform..
Specific Gravity 0.922 g/cc
0.922 g/cc
ASTM D792
Polymax® Maxelast® A9950C TPE, ABS/PC Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform..
Specific Gravity 0.922 g/cc
0.922 g/cc
ASTM D792
Polymax® Maxelast® A9960C TPE, ABS/PC Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform..
Specific Gravity 0.922 g/cc
0.922 g/cc
ASTM D792
Polymax® Maxelast® C4630 TPE, Transparent
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf..
Specific Gravity 0.922 g/cc
0.922 g/cc
ASTM D792
Polymax® Maxelast® C4640 TPE, Transparent
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf..
Specific Gravity 0.922 g/cc
0.922 g/cc
ASTM D792
Polymax® Maxelast® C4650 TPE, Transparent
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf..
Specific Gravity 0.922 g/cc
0.922 g/cc
ASTM D792
Polymax® Maxelast® P3970 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Specific Gravity 0.922 g/cc
0.922 g/cc
ASTM D792
Polymax® Maxelast® P3970H TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Specific Gravity 0.922 g/cc
0.922 g/cc
ASTM D792
Polymax® Maxelast® P3975H TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Specific Gravity 0.922 g/cc
0.922 g/cc
ASTM D792
Polymax® Maxelast® P3980H TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Specific Gravity 0.922 g/cc
0.922 g/cc
ASTM D792
Polymax® Maxelast® P3990H TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Specific Gravity 0.922 g/cc
0.922 g/cc
ISO 1183
Polimeri Europa Flexirene® MS 20 U Linear Low Density Polyethylene
Flexirene MS 20 U is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MS 20 U are characterized by optimum low tempe..
Specific Gravity 0.922 g/cc
0.922 g/cc
ISO 1183
Polimeri Europa Riblene® FC 26 Low Density Polyethylene - Blown Film Extrusion
Riblene FC 26 is a high molecular weight low density polyethylene (LDPE), with added antiblocking agent, suitable for blown film extrusion. Riblene FC 26 is characterized by a high melt strength le..
Specific Gravity 0.922 g/cc
0.922 g/cc
ISO 1183
Polimeri Europa Riblene® FC 30 Low Density Polyethylene - Blown Film Extrusion
Riblene FC 30 is a high molecular weight low density polyethylene resin (LDPE) suitable for blown film extrusion. Riblene FC 30 is characterized by a high melt strength leading to a good bubble sta..
Specific Gravity 0.922 g/cc
0.922 g/cc
ISO 1183-D
LG Chemical LUTENE XL8080NT PE Compound
Description: LUTENE XL8080NT is a standard version having excellent electrical properties for medium and high voltage power cable insulation and has a very low level of contamination.Applications: M..
Specific Gravity 0.922 - 0.926 g/cc
0.922 - 0.926 g/cc
ASTM D1505
LG Chemical SEETEC BF415 LDPE
Characteristics: Good Processability and Excellent Optical Properties Applications: Masking filmCAS No. 9002-88-4Information provided by LG Chemical
Specific Gravity 0.922 g/cc
0.922 g/cc
ASTM 792
Multibase Multi-Flex® D 5308 Platinum TPO Thermoplastic Polyolefin Elastomer
Forms: PelletsInformation provided by Multibase
Specific Gravity 0.922 g/cc
0.922 g/cc
ISO 1183-D
LG Chemical LUTENE XL8080UC PE Compound
Description: LUTENE XL8080UC is a superior cleanliness version for high voltage power cable insulation and is designated as UC (Ultra-Clean) due to its extremely low level of contamination. LUTENE X..
Specific Gravity 0.922 g/cc
0.922 g/cc
ASTM D792
Teknor Apex Telcar® TL-1155B Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Specific Gravity 0.922 g/cc
0.922 g/cc
ASTM D792
A. Schulman CP80-01 Linear Low-Density Polyethylene
DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In..
Specific Gravity 0.922 g/cc
0.922 g/cc
ASTM D792
A. Schulman CP80-01 Linear Low-Density Polyethylene
DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In..
Specific Gravity 0.922 g/cc
0.922 g/cc
ASTM D792
A. Schulman CP80-01 Linear Low-Density Polyethylene
DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In..
Specific Gravity 0.922 g/cc
0.922 g/cc
15°C
ExxonMobil SAE 40 Mobilgard M50
Mobilgard M50 by ExxonMobil is a premium, extra high performance 50 TBN engine oil designed for use in the most severe residual-fuelled medium-speed diesel applications found in marine and stationar..
Specific Gravity 0.922 g/cc
0.922 g/cc
ASTM D792
A. Schulman CP80-01 Linear Low-Density Polyethylene
DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In..
Specific Gravity 0.922 g/cc
0.922 g/cc
ASTM D792
A. Schulman CP80-01 Linear Low-Density Polyethylene
DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In..
Specific Gravity 0.922 g/cc
0.922 g/cc
ASTM D792
A. Schulman CP80-01 Linear Low-Density Polyethylene
DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In..
Specific Gravity 0.922 g/cc
0.922 g/cc
15°C
ExxonMobil SAE 40 Mobilgard M50
Mobilgard M50 by ExxonMobil is a premium, extra high performance 50 TBN engine oil designed for use in the most severe residual-fuelled medium-speed diesel applications found in marine and stationar..
Specific Gravity 0.922 g/cc
0.922 g/cc
ASTM D1505/D792
Braskem CX7020 Cast Film Extrusion Low Density Polyethylene
Smooth or embossed films for diapers, disposable sheets, etc. Films for lamination, Injection-Blow Molding, Foamed applications.Information provided by Braskem.
Specific Gravity 0.922 g/cc
0.922 g/cc
ASTM D1505/D792
Braskem F2022/0 Cast Film Extrusion Low Density Polyethylene
Films for diapers and absorbent articles; Medium resistance films or for general use.Information provided by Braskem.
Specific Gravity 0.922 g/cc
0.922 g/cc
ASTM D1505/D792
Braskem PB681/59 Blown Film Extrusion Low Density Polyethylene
Description: PB681/59 is a grade produced under high pressure in a tubular reactor. This resin is used for laminating films mainly on paper substrate. It is also used in the extrusion coating proces..