Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.918 - 0.921 g/cc | 0.918 - 0.921 g/cc | ASTM D1505 |
LG Chemical SEETEC BS500 LDPE Characteristics: Good Processability and Good cell uniformity& stability Additives: Antioxidant, Antiblocking agent, Slip AgentApplications: Foam sheetInformation provided by LG Chemical |
|||
Specific Gravity | 0.915 - 0.921 g/cc @Temperature 25.0 °C |
0.915 - 0.921 g/cc @Temperature 77.0 °F |
ASTM D4052 |
PolyOne Synplast™ DINA-N Di Isononyl Adipate Branched C9 adipate esterInformation provided by PolyOne |